Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.132 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.146 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.061 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 1> | 287.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 209.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 87.1 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 133.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 137.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 173.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 203.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 196.9 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 156.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 242.9 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 0> | 319.6 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 228.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 207.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 34.4 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 209.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 242.9 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 44.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 171.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 104.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 242.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 203.3 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 1> | 287.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 138.8 |
KCl (mp-23193) | <1 0 0> | <1 -1 0> | 319.6 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 228.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 232.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 259.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 319.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 310.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 277.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 259.1 |
InAs (mp-20305) | <1 0 0> | <1 -1 0> | 319.6 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 228.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 203.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 208.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 312.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 157.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 65.6 |
CdS (mp-672) | <1 1 0> | <1 -1 -1> | 298.5 |
LiF (mp-1138) | <1 0 0> | <1 -1 0> | 182.6 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 262.2 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 191.5 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 262.6 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 181.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 173.5 |
Te2W (mp-22693) | <0 1 1> | <1 -1 1> | 239.4 |
Te2W (mp-22693) | <0 0 1> | <1 -1 1> | 239.4 |
Te2W (mp-22693) | <0 1 0> | <1 -1 1> | 335.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.15265 | 0.07194 | 0.19999 | 0.00693 | -0.04056 | -0.01369 |
0.01388 | -0.01558 | 0.05245 | -0.05394 | -0.00856 | 0.02835 |
0.05144 | -0.04138 | -0.05273 | 0.02466 | 0.03572 | -0.05166 |
Piezoelectric Modulus ‖eij‖max0.27021 C/m2 |
Crystallographic Direction vmax |
---|
-9.00000 |
2.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.28 | -0.04 | -0.03 |
-0.04 | 2.25 | -0.03 |
-0.03 | -0.03 | 2.28 |
Dielectric Tensor εij (total) |
||
---|---|---|
4.42 | -0.25 | -0.21 |
-0.25 | 4.01 | -0.25 |
-0.21 | -0.25 | 4.32 |
Polycrystalline dielectric constant
εpoly∞
2.27
|
Polycrystalline dielectric constant
εpoly
4.25
|
Refractive Index n1.51 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsAuO3 (mp-755240) | 0.5847 | 0.117 | 3 |
VBO4 (mp-771386) | 0.6193 | 0.068 | 3 |
AlPO4 (mp-558088) | 0.6070 | 0.025 | 3 |
AlPO4 (mp-667310) | 0.5805 | 0.022 | 3 |
H2SeO4 (mp-626024) | 0.6359 | 0.002 | 3 |
LiNi(PO3)3 (mp-863900) | 0.7079 | 0.119 | 4 |
CsSi3HO7 (mp-758180) | 0.5488 | 0.002 | 4 |
CsSi2HO5 (mp-557780) | 0.6561 | 0.005 | 4 |
RbP(HO2)2 (mp-703528) | 0.6825 | 0.007 | 4 |
K2Zn(Si2O5)2 (mp-555568) | 0.7379 | 0.000 | 4 |
SiO2 (mp-556963) | 0.4355 | 0.144 | 2 |
SiO2 (mp-556994) | 0.4447 | 0.083 | 2 |
SiO2 (mp-558564) | 0.4440 | 0.064 | 2 |
SiO2 (mp-558569) | 0.4278 | 0.073 | 2 |
CeSe2 (mp-1080866) | 0.4247 | 0.504 | 2 |
RbB2P2HO9 (mp-758281) | 0.5364 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.7703 eV |
Corrected Energy-98.8621 eV
-98.8621 eV = -93.2438 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)