Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.257 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.670 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 1> | 202.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 202.6 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 79.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 285.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 285.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 106.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 79.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 285.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 214.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 213.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 79.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 316.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 214.4 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 257.2 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 101.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 213.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 285.8 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 128.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 285.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 158.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 142.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 237.7 |
Al (mp-134) | <1 1 0> | <1 1 1> | 257.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 214.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 285.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 101.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 237.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 285.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 237.7 |
C (mp-66) | <1 0 0> | <0 1 0> | 316.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 142.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 316.9 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 0> | 213.4 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 285.8 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 214.4 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 214.4 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 316.9 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 316.9 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 316.9 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 285.8 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 142.9 |
TbScO3 (mp-31119) | <1 1 1> | <1 1 0> | 213.4 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 158.5 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 79.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 79.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 101.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 213.4 |
Au (mp-81) | <1 0 0> | <0 1 0> | 158.5 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 79.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.4104 | 0.003 | 3 |
AlPO4 (mp-557362) | 0.3983 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.3685 | 0.011 | 3 |
Be(PO3)2 (mp-560521) | 0.4024 | 0.003 | 3 |
AlPO4 (mp-1019510) | 0.3468 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.5602 | 0.000 | 4 |
CsAlSiO4 (mp-561457) | 0.5924 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.6280 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.6097 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5813 | 0.000 | 4 |
SiO2 (mp-972808) | 0.2187 | 0.005 | 2 |
SiO2 (mp-11684) | 0.2179 | 0.040 | 2 |
CeSe2 (mp-1080278) | 0.2370 | 0.516 | 2 |
CeSe2 (mp-1080633) | 0.1586 | 0.516 | 2 |
CrN2 (mp-1096910) | 0.2461 | 0.389 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8949 eV |
Corrected Energy-401.4270 eV
-401.4270 eV = -378.9537 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|