Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.264 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.590 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 235.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 136.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 235.9 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 268.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 179.2 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 299.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 245.7 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 268.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 136.5 |
BN (mp-984) | <0 0 1> | <1 -1 0> | 299.6 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 268.8 |
BN (mp-984) | <1 1 0> | <0 1 1> | 136.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 314.5 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 179.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 235.9 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 299.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 239.5 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 136.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 157.3 |
TiO2 (mp-2657) | <0 0 1> | <1 -1 0> | 299.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 314.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 244.3 |
InSb (mp-20012) | <1 0 0> | <1 -1 0> | 299.6 |
PbSe (mp-2201) | <1 1 0> | <0 1 -1> | 268.8 |
PbSe (mp-2201) | <1 1 1> | <0 1 1> | 136.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 -1 1> | 118.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 314.5 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 157.3 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 136.5 |
Au (mp-81) | <1 0 0> | <0 1 0> | 245.7 |
CdSe (mp-2691) | <1 1 1> | <0 1 1> | 136.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 162.8 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 314.5 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 235.9 |
SiC (mp-8062) | <1 1 0> | <0 1 -1> | 268.8 |
CdWO4 (mp-19387) | <0 1 0> | <1 -1 1> | 237.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 314.5 |
CdTe (mp-406) | <1 0 0> | <1 -1 0> | 299.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 235.9 |
Ni (mp-23) | <1 1 0> | <1 -1 -1> | 138.3 |
Ni (mp-23) | <1 1 1> | <1 -1 0> | 299.6 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 235.9 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 314.5 |
Au (mp-81) | <1 1 0> | <0 1 -1> | 268.8 |
CdSe (mp-2691) | <1 1 0> | <0 1 -1> | 268.8 |
WS2 (mp-224) | <1 1 0> | <1 -1 0> | 299.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 244.3 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 244.3 |
TiO2 (mp-390) | <0 0 1> | <1 1 1> | 174.7 |
TiO2 (mp-390) | <1 0 0> | <0 1 -1> | 268.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BePO4 (mp-760410) | 0.3648 | 0.063 | 3 |
AlPO4 (mp-554273) | 0.3580 | 0.013 | 3 |
AlPO4 (mp-707977) | 0.3375 | 0.010 | 3 |
AlPO4 (mp-541338) | 0.3584 | 0.012 | 3 |
AlPO4 (mp-561027) | 0.3318 | 0.012 | 3 |
CsBeAsO4 (mp-9113) | 0.6119 | 0.000 | 4 |
KAlSi3O8 (mp-697670) | 0.7019 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.5787 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.7167 | 0.000 | 4 |
Rb2MgSi5O12 (mp-1020860) | 0.6519 | 0.000 | 4 |
SiO2 (mp-600072) | 0.1759 | 0.014 | 2 |
SiO2 (mp-559360) | 0.1300 | 0.009 | 2 |
SiO2 (mp-560941) | 0.1588 | 0.011 | 2 |
SiO2 (mp-600015) | 0.1829 | 0.011 | 2 |
CeSe2 (mp-1080642) | 0.1848 | 0.522 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9025 eV |
Corrected Energy-301.3453 eV
-301.3453 eV = -284.4904 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)