Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.757 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.521 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap2.536 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nnc [126] |
HallP 4 2 1n |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 127.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 139.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 139.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 254.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 174.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 174.7 |
BN (mp-984) | <1 0 0> | <1 1 0> | 247.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 291.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 174.7 |
Al (mp-134) | <1 1 0> | <1 0 1> | 139.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 82.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 164.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 174.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 127.2 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 139.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 139.9 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 247.1 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 233.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 291.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 291.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 233.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 233.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 127.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 164.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 127.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 127.2 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 139.9 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 82.4 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 58.2 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 247.1 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 164.7 |
GaP (mp-2490) | <1 0 0> | <1 1 0> | 247.1 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 174.7 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 127.2 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 127.2 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 233.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 174.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 127.2 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 291.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 174.7 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 174.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 174.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 82.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 116.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 127.2 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 291.2 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 164.7 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 0> | 174.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 58.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 174.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SiO2 (mp-557814) | 0.7147 | 0.706 | 2 |
CeSe2 (mp-1080358) | 0.6902 | 0.551 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.3952 eV |
Corrected Energy-377.4439 eV
-377.4439 eV = -354.9706 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|