Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.142 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnS |
Band Gap2.011 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 321.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 347.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 167.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 373.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 283.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 308.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 270.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 193.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 167.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 115.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 257.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 334.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 167.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 128.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 308.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 90.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 51.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 12.9 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 115.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 38.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 257.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 102.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 90.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 270.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 193.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 115.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 270.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 308.7 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 308.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 321.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 270.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 270.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 193.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 205.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 257.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 360.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 205.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 321.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 270.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 205.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si3NiP4 (mp-8311) | 0.1876 | 0.000 | 3 |
Cu2SiTe3 (mp-675120) | 0.1881 | 0.001 | 3 |
Li3SbS4 (mp-760415) | 0.1822 | 0.005 | 3 |
GaCuTe2 (mp-3839) | 0.1887 | 0.000 | 3 |
CrCd3Te4 (mp-1079533) | 0.1854 | 0.295 | 3 |
CoCu2SiS4 (mp-556830) | 0.1773 | 0.065 | 4 |
FeCu2SiSe4 (mp-1025510) | 0.1837 | 0.223 | 4 |
ZnCu2GeS4 (mp-6408) | 0.1659 | 0.000 | 4 |
CoCu2SiS4 (mp-11769) | 0.1743 | 0.065 | 4 |
ZnCu2SiTe4 (mp-1078498) | 0.1817 | 0.000 | 4 |
ZnS (mp-556363) | 0.0023 | 0.001 | 2 |
ZnS (mp-557346) | 0.0023 | 0.001 | 2 |
ZnS (mp-557175) | 0.0022 | 0.001 | 2 |
ZnS (mp-555773) | 0.0026 | 0.001 | 2 |
ZnS (mp-556152) | 0.0026 | 0.001 | 2 |
C (mp-611448) | 0.0334 | 0.143 | 1 |
C (mp-616440) | 0.0216 | 0.141 | 1 |
C (mp-569517) | 0.0458 | 0.145 | 1 |
C (mp-569567) | 0.0244 | 0.144 | 1 |
Ge (mp-1091415) | 0.0805 | 0.014 | 1 |
Explore more synthesis descriptions for materials of composition ZnS.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn S |
Final Energy/Atom-3.5087 eV |
Corrected Energy-138.2561 eV
-138.2561 eV = -126.3138 eV (uncorrected energy) - 11.9423 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)