Final Magnetic Moment0.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.296 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.290 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeCl3 + FeS2 + SCl + N2 |
Band Gap0.551 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 259.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 259.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 259.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 180.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 90.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 180.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 270.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 172.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 180.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 259.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 259.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 259.2 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 90.1 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 172.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 180.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 180.2 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 270.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 270.4 |
Au (mp-81) | <1 1 0> | <0 0 1> | 270.4 |
C (mp-48) | <1 1 0> | <0 1 0> | 259.2 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 270.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 -1> | 187.4 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 270.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
S5N4O3 (mp-540558) | 0.4740 | 0.199 | 3 |
S7(N3O4)2 (mp-28474) | 0.6602 | 0.232 | 3 |
P2CN3Cl5 (mp-662643) | 0.6727 | 0.051 | 4 |
FeS4N4Cl3 (mp-557331) | 0.1603 | 0.294 | 4 |
PCN2Cl3 (mp-650336) | 0.6146 | 0.058 | 4 |
BS4N4F3 (mp-16813) | 0.3052 | 0.111 | 4 |
H6S(NO2)2 (mp-721268) | 0.6483 | 0.320 | 4 |
NaSi2BH2O7 (mp-867930) | 0.7002 | 0.102 | 5 |
ZnH8C4(NO3)2 (mp-655017) | 0.7440 | 0.584 | 5 |
CS5N5O3F (mp-558959) | 0.4468 | 0.213 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv S N Cl |
Final Energy/Atom-5.1236 eV |
Corrected Energy-256.5497 eV
-256.5497 eV = -245.9343 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)