Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.483 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.162 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 233.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 141.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 134.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 202.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 93.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 269.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 280.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 141.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 280.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 311.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 233.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 141.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 280.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 141.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 187.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 187.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 233.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 269.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 77.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 233.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 311.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 202.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 -1> | 237.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 233.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 280.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 280.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 187.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 233.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 230.5 |
C (mp-66) | <1 1 0> | <1 0 -1> | 292.7 |
TiO2 (mp-2657) | <1 0 0> | <1 1 -1> | 237.1 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 280.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 233.6 |
Mg (mp-153) | <0 0 1> | <1 1 -1> | 237.1 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 205.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 202.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 311.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 280.7 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 280.7 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 97.6 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 311.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 187.1 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 233.6 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 93.6 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 269.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 311.4 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 233.6 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 155.7 |
WS2 (mp-224) | <0 0 1> | <1 1 -1> | 237.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2(CO3)3 (mp-762590) | 0.5769 | 0.280 | 3 |
Co2(CO3)3 (mp-997509) | 0.5960 | 0.189 | 3 |
Zn(NO3)2 (mp-778973) | 0.5912 | 0.007 | 3 |
Mn2(CO3)3 (mp-762671) | 0.6130 | 0.060 | 3 |
Zn(CO2)2 (mp-559437) | 0.6137 | 0.059 | 3 |
LiV(CO3)2 (mp-765385) | 0.6290 | 0.065 | 4 |
CuHCO4 (mp-769935) | 0.6248 | 0.044 | 4 |
VH4(CO3)2 (mp-601574) | 0.5690 | 0.124 | 4 |
ZnH4(NO4)2 (mp-696291) | 0.6358 | 0.000 | 4 |
CoHCO4 (mp-1022803) | 0.6257 | 0.087 | 4 |
CuH10C2(N2O5)2 (mp-601396) | 0.6968 | 0.284 | 5 |
K2VH4C4O9 (mp-601777) | 0.4450 | 0.135 | 5 |
NaSbCO2F3 (mp-554239) | 0.6806 | 0.031 | 5 |
NaSbCO2F3 (mp-554716) | 0.6841 | 0.031 | 5 |
CuH8C4(NO3)2 (mp-560533) | 0.6640 | 0.161 | 5 |
FeH16C4S4(N4Cl)2 (mp-723036) | 0.7317 | 0.101 | 6 |
CdH16C4S4(N4Cl)2 (mp-699261) | 0.7004 | 0.033 | 6 |
MnH18C4N8(ClO)4 (mp-735514) | 0.7446 | 0.082 | 6 |
CdH4CN2Cl2O (mp-697033) | 0.6276 | 0.000 | 6 |
CoH18C4N8(ClO)4 (mp-744629) | 0.7380 | 0.036 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Cu_pv C O |
Final Energy/Atom-6.2780 eV |
Corrected Energy-292.7194 eV
Uncorrected energy = -276.2314 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -292.7194 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)