Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.449 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK3NO4 + KNO3 + Na2O |
Band Gap4.048 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 241.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 314.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 167.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 175.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 167.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 314.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 209.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 209.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 157.4 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 254.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 209.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 115.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 120.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 52.5 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 231.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 209.8 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 167.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 1> | 175.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 314.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 262.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 262.3 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 314.7 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 241.0 |
BN (mp-984) | <0 0 1> | <1 0 1> | 131.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 120.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 262.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 209.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 209.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 167.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 241.0 |
C (mp-66) | <1 0 0> | <0 1 1> | 127.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 314.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 231.9 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 262.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 314.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 209.8 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 231.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 115.9 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 262.9 |
C (mp-66) | <1 1 1> | <1 1 1> | 175.3 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 167.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 231.9 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 104.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 52.5 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 314.7 |
WS2 (mp-224) | <1 1 0> | <0 1 0> | 231.9 |
C (mp-48) | <1 0 1> | <1 0 0> | 120.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 209.8 |
WSe2 (mp-1821) | <1 1 0> | <1 0 1> | 262.9 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 314.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2RuO4 (mp-17789) | 0.5737 | 0.000 | 3 |
Rb3PO4 (mp-558170) | 0.5993 | 0.000 | 3 |
Cs3NO4 (mp-768311) | 0.5916 | 0.034 | 3 |
K3NO4 (mp-28202) | 0.5728 | 0.000 | 3 |
Cs3PO4 (mp-559808) | 0.5687 | 0.000 | 3 |
Cd2H2SO6 (mp-634113) | 0.6050 | 0.003 | 4 |
GaHg2SbCl4 (mp-568031) | 0.5677 | 0.001 | 4 |
Na2Cd(SO4)2 (mp-558198) | 0.6087 | 0.000 | 4 |
AlHg2SbCl4 (mp-570828) | 0.5720 | 0.000 | 4 |
Na3Ce(PO4)2 (mp-556334) | 0.6250 | 0.000 | 4 |
SrCaSn(PO4)2 (mvc-2825) | 0.6384 | 0.052 | 5 |
SrCaMn(PO4)2 (mvc-3008) | 0.6920 | 0.014 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Na_pv N O |
Final Energy/Atom-5.0199 eV |
Corrected Energy-343.2552 eV
Uncorrected energy = -321.2712 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Corrected energy = -343.2552 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)