Final Magnetic Moment15.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFerri |
Formation Energy / Atom-2.042 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoO2 + Mo8O23 |
Band Gap0.016 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPba2 [32] |
HallP 2 2ab |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 237.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 263.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 263.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 160.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 240.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 240.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 240.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 240.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 175.3 |
BN (mp-984) | <1 1 0> | <0 1 1> | 237.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 160.0 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 263.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 263.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 240.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 263.0 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 263.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 160.0 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 263.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 160.0 |
Si (mp-149) | <1 1 1> | <0 0 1> | 160.0 |
C (mp-48) | <1 0 1> | <0 1 0> | 263.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 160.0 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 160.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 80.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 118.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 240.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 240.1 |
C (mp-48) | <1 0 0> | <0 1 0> | 175.3 |
C (mp-48) | <1 1 0> | <0 1 1> | 237.4 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 160.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 240.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 263.0 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 160.0 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 240.1 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 263.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
W18O49 (mp-19529) | 0.6052 | 0.001 | 2 |
W8O21 (mp-579377) | 0.6185 | 0.004 | 2 |
W18O49 (mp-567091) | 0.6069 | 0.000 | 2 |
Li3Zr4F19 (mp-29040) | 0.7373 | 0.000 | 3 |
Sr3U11O36 (mp-667349) | 0.7028 | 0.000 | 3 |
Ta2WO8 (mp-773933) | 0.6676 | 0.000 | 3 |
Li3V4F19 (mp-776830) | 0.7282 | 0.070 | 3 |
K2Mo7O20 (mp-579220) | 0.7122 | 0.007 | 3 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points3 |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv O |
Final Energy/Atom-7.0977 eV |
Corrected Energy-1094.5766 eV
-1094.5766 eV = -908.5074 eV (uncorrected energy) - 120.0540 eV (MP Advanced Correction) - 66.0153 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)