Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.392 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAsS + As |
Band Gap2.485 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 1 0> | 262.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 234.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 174.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 156.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 87.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 234.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 262.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 153.5 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 117.3 |
C (mp-66) | <1 0 0> | <1 0 1> | 153.5 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 234.5 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 234.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 156.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 234.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 234.5 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 132.1 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 262.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 262.3 |
Si (mp-149) | <1 0 0> | <0 0 1> | 234.5 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 234.5 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 132.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 262.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 87.4 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 234.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 234.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 234.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 234.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 156.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 117.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 234.5 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 234.5 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 132.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 264.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 234.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 234.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 78.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 78.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 234.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 262.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 312.7 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 234.6 |
WS2 (mp-224) | <1 1 0> | <1 0 1> | 153.5 |
C (mp-48) | <0 0 1> | <1 1 0> | 158.4 |
C (mp-48) | <1 0 1> | <0 1 0> | 262.3 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 234.5 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 158.4 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 78.2 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 262.3 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 132.1 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 234.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sb5S3O5 (mvc-12918) | 0.7498 | 0.138 | 3 |
TlAs5S8 (mp-28442) | 0.6979 | 0.006 | 3 |
TlHg(AsS2)3 (mp-6096) | 0.6245 | 0.003 | 4 |
As4S3 (mp-27543) | 0.2743 | 0.004 | 2 |
AsS (mp-542604) | 0.4323 | 0.026 | 2 |
AsS (mp-556328) | 0.3893 | 0.023 | 2 |
P4S3 (mp-1468) | 0.4379 | 0.000 | 2 |
P4S3 (mp-1469) | 0.2758 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: As S |
Final Energy/Atom-4.5429 eV |
Corrected Energy-135.1630 eV
-135.1630 eV = -127.2015 eV (uncorrected energy) - 7.9615 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)