Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.592 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.355 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdTe (mp-406) | <1 0 0> | <0 0 1> | 269.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 161.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 136.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 226.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 136.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 226.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 136.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 269.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 323.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 215.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 53.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 215.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 269.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 161.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 136.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 113.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 323.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 323.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 269.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 323.1 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 323.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 215.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 136.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 53.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 323.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 136.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 113.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 113.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 269.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 161.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 113.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 215.4 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 136.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 53.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 323.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 269.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 323.1 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 269.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 269.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 161.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 323.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 161.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 215.4 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 113.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 269.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 215.4 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 215.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi6P2O15 (mp-767410) | 0.5819 | 0.069 | 3 |
P2Pb4O9 (mp-31068) | 0.5825 | 0.000 | 3 |
Pb3SO6 (mp-559143) | 0.5758 | 0.004 | 3 |
Ga(BiBr)4 (mp-571502) | 0.5702 | 0.008 | 3 |
Bi3(PO5)2 (mvc-15217) | 0.5310 | 0.070 | 3 |
RbEuPO4 (mp-18169) | 0.5871 | 0.007 | 4 |
BaLa2BeO5 (mp-18414) | 0.5946 | 0.000 | 4 |
Rb12Sn8GeO4 (mp-680377) | 0.5530 | 0.005 | 4 |
AlSb2(TeCl2)2 (mp-567743) | 0.5286 | 0.000 | 4 |
H2Pb4SO8 (mp-697676) | 0.5399 | 0.001 | 4 |
GaBr2 (mp-650841) | 0.7463 | 0.010 | 2 |
KBiS(ClO2)2 (mp-23645) | 0.5991 | 0.000 | 5 |
KSnSO4F (mp-557399) | 0.6352 | 0.000 | 5 |
CuTe4H12C4N (mp-570909) | 0.6868 | 0.092 | 5 |
CaGdTh(PO4)3 (mp-695308) | 0.6716 | 0.016 | 5 |
Tl3Hg2S3ClO12 (mp-554279) | 0.6638 | 0.000 | 5 |
Na2LiCaVP2O9 (mp-763838) | 0.7298 | 0.090 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sb S O F |
Final Energy/Atom-5.2170 eV |
Corrected Energy-326.9089 eV
-326.9089 eV = -313.0185 eV (uncorrected energy) - 13.8905 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)