Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.115 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.632 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <1 0 0> | 134.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 134.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 134.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 134.4 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 134.4 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 134.4 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 134.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.1934 | 0.012 | 3 |
AlPO4 (mp-554273) | 0.2484 | 0.013 | 3 |
AlPO4 (mp-557604) | 0.1870 | 0.010 | 3 |
AlPO4 (mp-683883) | 0.0889 | 0.018 | 3 |
AlPO4 (mp-561027) | 0.2358 | 0.012 | 3 |
CsBeAsO4 (mp-9113) | 0.5089 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.6066 | 0.002 | 4 |
CsFeSiO4 (mp-644325) | 0.6129 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.4838 | 0.000 | 4 |
Rb2MgSi5O12 (mp-1020860) | 0.5638 | 0.000 | 4 |
SiO2 (mp-600070) | 0.3199 | 0.017 | 2 |
SiO2 (mp-600057) | 0.3131 | 0.018 | 2 |
SiO2 (mp-669426) | 0.3363 | 0.005 | 2 |
SiO2 (mp-600059) | 0.3075 | 0.011 | 2 |
SiO2 (mp-556262) | 0.3484 | 0.015 | 2 |
CsZnB(PO4)2 (mp-560244) | 0.7280 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.4724 eV |
Corrected Energy-570.9896 eV
Uncorrected energy = -538.0136 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Corrected energy = -570.9896 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)