Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.805 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNO2 |
Band Gap2.875 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3 [204] |
Hall-I 2 2 3 |
Point Groupm3 |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 212.0 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 299.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 74.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 106.0 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 129.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 224.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 224.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 74.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 106.0 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 149.9 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 106.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 74.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 106.0 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 212.0 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 299.7 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 212.0 |
Si (mp-149) | <1 0 0> | <1 0 0> | 149.9 |
Au (mp-81) | <1 0 0> | <1 1 1> | 259.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 74.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 106.0 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 299.7 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 224.8 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 149.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 149.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 299.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 106.0 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 149.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 74.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 106.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 299.7 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 299.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 149.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 212.0 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 74.9 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 106.0 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 149.9 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 299.7 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 259.6 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 224.8 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 299.7 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 149.9 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 224.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 224.8 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 74.9 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 106.0 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 299.7 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 212.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.96 | -0.00 | 0.00 |
-0.00 | 1.96 | -0.00 |
0.00 | -0.00 | 1.96 |
Dielectric Tensor εij (total) |
||
---|---|---|
2.29 | -0.00 | 0.00 |
-0.00 | 2.29 | -0.00 |
0.00 | -0.00 | 2.29 |
Polycrystalline dielectric constant
εpoly∞
1.96
|
Polycrystalline dielectric constant
εpoly
2.29
|
Refractive Index n1.40 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaClO3 (mp-630949) | 0.5843 | 0.615 | 3 |
CCl2O (mp-27727) | 0.5341 | 0.015 | 3 |
TlHO (mp-626647) | 0.6776 | 0.033 | 3 |
Fe(NF2)3 (mp-1095055) | 0.7085 | 0.784 | 3 |
TlNO3 (mp-662551) | 0.7120 | 0.701 | 3 |
H4CN2O (mp-976707) | 0.6343 | 0.023 | 4 |
H4CSN2 (mp-735023) | 0.7385 | 0.010 | 4 |
BF2 (mp-27864) | 0.4226 | 0.121 | 2 |
BF3 (mp-27896) | 0.6079 | 0.000 | 2 |
BF3 (mp-558149) | 0.6075 | 0.000 | 2 |
NO2 (mp-2789) | 0.4263 | 0.000 | 2 |
NO2 (mp-1771) | 0.2805 | 0.001 | 2 |
Explore more synthesis descriptions for materials of composition NO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: N O |
Final Energy/Atom-6.2862 eV |
Corrected Energy-121.5790 eV
-121.5790 eV = -113.1515 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)