Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.516 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.789 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 233.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 193.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 141.6 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 0> | 312.8 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 230.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 193.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 233.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 -1 0> | 125.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 235.9 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 344.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 204.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 238.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 193.9 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 0> | 125.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 173.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 288.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 262.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 321.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 220.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 116.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 262.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 344.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 262.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 178.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 264.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 233.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 188.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 146.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 232.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 193.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 321.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 288.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 321.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 204.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 0> | 250.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 230.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 193.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 115.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 344.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 297.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 271.4 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 230.6 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 269.0 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 230.6 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 115.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 193.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 147.6 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 115.3 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 221.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 330.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg7(PO5)2 (mp-29958) | 0.6393 | 0.000 | 3 |
Al2Hg3Cl8 (mp-27346) | 0.6058 | 0.000 | 3 |
CrAgO4 (mp-849702) | 0.6549 | 0.423 | 3 |
NaPO3 (mp-648072) | 0.6454 | 0.050 | 3 |
Hg3PO4 (mp-554914) | 0.5736 | 0.000 | 3 |
SnPHO4 (mp-690702) | 0.5779 | 0.000 | 4 |
AgH2ClO5 (mp-24053) | 0.6384 | 0.002 | 4 |
Tl2CuAsO4 (mp-559727) | 0.4405 | 0.019 | 4 |
Tl2CuAsO4 (mp-558338) | 0.4835 | 0.006 | 4 |
Na2PH5O6 (mp-698223) | 0.5448 | 0.034 | 4 |
Na3Zn4As3H12O19 (mp-850445) | 0.6455 | 0.018 | 5 |
CsBaSiHO4 (mp-995225) | 0.6729 | 0.045 | 5 |
K4PH5Se3O16 (mp-695043) | 0.6743 | 0.000 | 5 |
K4PH5Se3O16 (mp-677734) | 0.6749 | 0.000 | 5 |
CaZnSiH2O5 (mp-696853) | 0.6370 | 0.004 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.6922 | 0.016 | 6 |
KLiPH2O4F (mp-690708) | 0.7461 | 0.039 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv As Pb_d O |
Final Energy/Atom-5.7164 eV |
Corrected Energy-85.6474 eV
-85.6474 eV = -80.0291 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|