Final Magnetic Moment1.022 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.008 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.217 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 195.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 85.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 170.1 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 258.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 85.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 170.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 255.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 255.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 255.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 292.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 85.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 195.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 97.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 97.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 97.5 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 292.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 292.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 292.6 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 292.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 129.4 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 195.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 97.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 170.1 |
Al (mp-134) | <1 0 0> | <0 1 0> | 97.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 255.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 85.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 255.1 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 292.6 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 97.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 255.1 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 170.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 97.5 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 292.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 195.1 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 258.8 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 85.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 255.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 97.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 258.8 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 85.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 85.0 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 1> | 258.8 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 195.1 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 255.1 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 255.1 |
Si (mp-149) | <1 1 0> | <0 0 1> | 85.0 |
Au (mp-81) | <1 0 0> | <0 1 0> | 292.6 |
C (mp-48) | <0 0 1> | <0 1 1> | 258.8 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 255.1 |
NaCl (mp-22862) | <1 0 0> | <0 1 0> | 97.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Mo4P5O24 (mp-705470) | 0.5669 | 0.022 | 4 |
Al4P3(HO5)3 (mp-706709) | 0.6734 | 0.027 | 4 |
KMnVO4 (mp-578924) | 0.6534 | 0.009 | 4 |
LiUAsO6 (mp-558717) | 0.6613 | 0.010 | 4 |
Fe4P3(HO5)3 (mp-25756) | 0.6580 | 0.000 | 4 |
Fe2CuAs2(HO5)2 (mp-764827) | 0.7224 | 0.283 | 5 |
NaAl3P2(HO3)4 (mp-706525) | 0.5641 | 0.006 | 5 |
NaGa3P2(HO3)4 (mp-759759) | 0.5860 | 0.008 | 5 |
ZrMn2Ag4(MoO4)6 (mp-581642) | 0.7408 | 0.000 | 5 |
ZnFe2As2(HO5)2 (mp-767897) | 0.7431 | 0.000 | 5 |
Ba3Li2Mo4P6(ClO14)2 (mp-699932) | 0.7316 | 0.005 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv Bi O |
Final Energy/Atom-6.5473 eV |
Corrected Energy-719.8580 eV
-719.8580 eV = -654.7274 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 20.1840 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)