Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.001 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.955 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 272.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 253.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 272.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 113.7 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 113.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 272.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 272.4 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 229.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 215.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 229.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 272.4 |
BN (mp-984) | <0 0 1> | <0 1 0> | 272.4 |
BN (mp-984) | <1 1 0> | <0 1 -1> | 133.7 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 272.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 272.4 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 272.4 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 227.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 -1 -1> | 192.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 1> | 220.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 1> | 220.6 |
TbScO3 (mp-31119) | <0 0 1> | <1 -1 -1> | 192.0 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 272.4 |
PbSe (mp-2201) | <1 1 0> | <1 1 1> | 110.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 253.8 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 110.3 |
SiC (mp-11714) | <1 0 1> | <1 1 0> | 229.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 113.7 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 0> | 272.4 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 1> | 113.7 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 272.4 |
CdSe (mp-2691) | <1 1 0> | <0 1 1> | 113.7 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 253.8 |
WS2 (mp-224) | <1 0 1> | <0 1 1> | 227.3 |
TiO2 (mp-390) | <1 1 1> | <0 1 0> | 272.4 |
C (mp-48) | <1 0 0> | <1 1 0> | 114.6 |
C (mp-48) | <1 0 1> | <0 1 0> | 181.6 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 -1> | 156.2 |
ZnO (mp-2133) | <1 0 0> | <1 0 1> | 228.8 |
ZnO (mp-2133) | <1 1 1> | <1 0 -1> | 156.2 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 272.4 |
GaSb (mp-1156) | <1 1 0> | <1 1 1> | 110.3 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 181.6 |
SiC (mp-8062) | <1 1 1> | <0 1 0> | 272.4 |
GaTe (mp-542812) | <0 0 1> | <0 1 1> | 227.3 |
GaTe (mp-542812) | <1 0 -1> | <0 1 1> | 227.3 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 220.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2Hg3Cl8 (mp-27346) | 0.7293 | 0.000 | 3 |
Rb14Si10O17 (mp-680306) | 0.7080 | 0.002 | 3 |
RbH3(SO4)2 (mp-733612) | 0.6020 | 0.000 | 4 |
K2PHO4 (mp-733468) | 0.5517 | 0.000 | 4 |
BaPHO4 (mp-698163) | 0.6156 | 0.001 | 4 |
HSeNO4 (mp-696797) | 0.5798 | 1.026 | 4 |
SrPHO4 (mp-735022) | 0.6222 | 0.001 | 4 |
KPHO3F (mp-758619) | 0.3607 | 0.000 | 5 |
K4PH5S3O16 (mp-677192) | 0.2546 | 0.000 | 5 |
K4PH5Se3O16 (mp-695043) | 0.3356 | 0.000 | 5 |
K4LiH3(SO4)4 (mp-709186) | 0.3412 | 0.000 | 5 |
K4PH5Se3O16 (mp-677734) | 0.3608 | 0.000 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.7408 | 0.016 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv As H S O |
Final Energy/Atom-5.5749 eV |
Corrected Energy-349.7971 eV
-349.7971 eV = -323.3430 eV (uncorrected energy) - 26.4540 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)