Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.126 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.589 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 234.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 199.3 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 199.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 234.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 58.5 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 99.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 292.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 175.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 263.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 119.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 175.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 199.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 175.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 168.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 175.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 292.6 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 299.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 234.0 |
BN (mp-984) | <1 1 1> | <0 1 0> | 235.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 175.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 292.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 299.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 292.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 -1> | 299.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 235.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 292.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 234.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 292.6 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 292.6 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 175.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 299.0 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 175.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 292.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 199.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 175.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 292.6 |
Au (mp-81) | <1 1 1> | <1 0 -1> | 299.0 |
CdSe (mp-2691) | <1 0 0> | <1 0 -1> | 199.3 |
WS2 (mp-224) | <1 0 1> | <1 0 0> | 234.0 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 234.0 |
C (mp-48) | <1 1 1> | <1 0 0> | 234.0 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 292.6 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 175.5 |
SiC (mp-8062) | <1 1 0> | <1 0 -1> | 299.0 |
MgF2 (mp-1249) | <0 0 1> | <1 0 -1> | 199.3 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 234.0 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 175.5 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 0> | 292.6 |
GaSb (mp-1156) | <1 0 0> | <1 0 -1> | 199.3 |
Cu (mp-30) | <1 1 0> | <0 1 1> | 168.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsGaBr4 (mp-672251) | 0.7421 | 0.000 | 3 |
Ga(BiBr)4 (mp-571502) | 0.7133 | 0.004 | 3 |
TlGaBr4 (mp-569348) | 0.7405 | 0.000 | 3 |
Ba3(PS4)2 (mp-554255) | 0.6778 | 0.000 | 3 |
CsGaCl4 (mp-608516) | 0.7353 | 0.000 | 3 |
NaNd(SO4)2 (mp-866078) | 0.6324 | 0.013 | 4 |
BaBi6(PO5)4 (mp-554084) | 0.7450 | 0.000 | 4 |
NaLa(SO4)2 (mp-557840) | 0.6635 | 0.000 | 4 |
NaPr2S2O8F3 (mp-560673) | 0.6158 | 0.000 | 5 |
Rb3Hg2S3ClO12 (mp-560324) | 0.7435 | 0.000 | 5 |
Tl3Hg2S3ClO12 (mp-554279) | 0.7440 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv La S O F |
Final Energy/Atom-6.6855 eV |
Corrected Energy-227.8256 eV
-227.8256 eV = -213.9351 eV (uncorrected energy) - 13.8905 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)