Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.106 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.025 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.634 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VBO4 (mp-771386) | 0.4232 | 0.068 | 3 |
AlPO4 (mp-557757) | 0.4525 | 0.016 | 3 |
AlPO4 (mp-683883) | 0.4282 | 0.018 | 3 |
CoPO4 (mp-771533) | 0.3663 | 0.019 | 3 |
AlPO4 (mp-667310) | 0.3177 | 0.022 | 3 |
CsSi3HO7 (mp-758180) | 0.4317 | 0.002 | 4 |
KAlSi3O8 (mp-697670) | 0.6114 | 0.000 | 4 |
LiB(SO4)2 (mp-1020106) | 0.6272 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.6109 | 0.000 | 4 |
Rb2MgSi5O12 (mp-1080284) | 0.5906 | 0.017 | 4 |
CrN2 (mp-1015026) | 0.4047 | 0.438 | 2 |
SiO2 (mp-556994) | 0.4379 | 0.083 | 2 |
SiO2 (mp-555147) | 0.4228 | 0.089 | 2 |
SiO2 (mp-558569) | 0.4025 | 0.073 | 2 |
CeSe2 (mp-1080636) | 0.4154 | 0.506 | 2 |
KBaAl3Si5O16 (mp-677121) | 0.7225 | 0.009 | 5 |
RbB2P2HO9 (mp-758281) | 0.7118 | 0.000 | 5 |
RbZnB(PO4)2 (mp-557658) | 0.7490 | 0.000 | 5 |
CsZnB(PO4)2 (mp-560244) | 0.6900 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.4625 eV |
Corrected Energy-856.5155 eV
-856.5155 eV = -805.9506 eV (uncorrected energy) - 50.5649 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)