Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 103.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 213.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 311.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 34.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 235.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 142.8 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 53.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 172.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 121.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 172.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 187.5 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 117.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 172.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 53.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 238.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 283.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 138.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 121.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 214.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 53.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 312.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 138.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 162.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 207.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 58.8 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 294.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 121.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 172.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 53.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 333.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 213.1 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 311.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 162.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 324.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 187.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 345.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 266.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 333.2 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 62.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 345.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 202.6 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 312.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 324.1 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 213.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 333.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 176.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 294.2 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 103.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 138.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 213.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
93 | 99 | 96 | 0 | 0 | 0 |
99 | 221 | 133 | 0 | 0 | 0 |
96 | 133 | 245 | 0 | 0 | 0 |
0 | 0 | 0 | 61 | 0 | 0 |
0 | 0 | 0 | 0 | 35 | 0 |
0 | 0 | 0 | 0 | 0 | 38 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
24.4 | -7.6 | -5.5 | 0 | 0 | 0 |
-7.6 | 9.1 | -1.9 | 0 | 0 | 0 |
-5.5 | -1.9 | 7.3 | 0 | 0 | 0 |
0 | 0 | 0 | 16.4 | 0 | 0 |
0 | 0 | 0 | 0 | 28.8 | 0 |
0 | 0 | 0 | 0 | 0 | 26.3 |
Shear Modulus GV42 GPa |
Bulk Modulus KV135 GPa |
Shear Modulus GR34 GPa |
Bulk Modulus KR93 GPa |
Shear Modulus GVRH38 GPa |
Bulk Modulus KVRH114 GPa |
Elastic Anisotropy1.60 |
Poisson's Ratio0.35 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InOF2 (mp-1066872) | 0.7217 | 0.345 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pd S |
Final Energy/Atom-5.1313 eV |
Corrected Energy-42.3772 eV
-42.3772 eV = -41.0502 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)