Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.488 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 -1> | 169.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 237.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 238.3 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 258.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 101.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 238.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 158.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 238.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 317.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 317.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 317.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 238.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 181.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 135.0 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 203.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 238.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 238.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 317.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 238.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 317.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 317.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 317.7 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 317.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 317.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 238.3 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 150.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 203.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 238.3 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 158.9 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 1> | 258.2 |
WS2 (mp-224) | <1 0 0> | <1 0 -1> | 135.0 |
C (mp-48) | <1 0 1> | <0 1 1> | 258.2 |
C (mp-48) | <1 1 1> | <0 0 1> | 238.3 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 158.9 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 238.3 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 317.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 317.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 238.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 238.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 158.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 317.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 238.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 158.9 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 1> | 258.2 |
WSe2 (mp-1821) | <1 0 0> | <0 1 1> | 258.2 |
WSe2 (mp-1821) | <1 0 1> | <0 1 1> | 258.2 |
NaCl (mp-22862) | <1 1 0> | <1 0 -1> | 135.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 203.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb2SeF14 (mp-27312) | 0.6153 | 0.000 | 3 |
Sb2TeF14 (mp-27473) | 0.6361 | 0.000 | 3 |
SbSCl9 (mp-557809) | 0.5752 | 0.000 | 3 |
Ge(SF6)2 (mp-28291) | 0.6430 | 0.000 | 3 |
USCl9 (mp-28103) | 0.5758 | 0.014 | 3 |
AsSe(IF2)3 (mp-559575) | 0.3818 | 0.006 | 4 |
SbS(BrF2)3 (mp-555288) | 0.1833 | 0.000 | 4 |
AsSe(ClF2)3 (mp-554706) | 0.4024 | 0.000 | 4 |
SbSe(IF2)3 (mp-558026) | 0.3597 | 0.000 | 4 |
SbS(BrF2)3 (mp-560639) | 0.3662 | 0.001 | 4 |
SbF4 (mp-556425) | 0.6874 | 0.000 | 2 |
HgSb4C2(OF11)2 (mp-556903) | 0.7332 | 0.080 | 5 |
FeCoH18(CN2)6 (mp-505732) | 0.7492 | 0.096 | 5 |
FeSb2WC8Se2(O2F3)4 (mp-651106) | 0.7437 | 0.379 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: As S Br F |
Final Energy/Atom-3.6403 eV |
Corrected Energy-162.8251 eV
-162.8251 eV = -160.1712 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)