Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.729 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.659 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 0 0> | 223.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 287.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 331.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 287.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 115.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 298.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 265.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 223.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 331.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 115.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 298.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 287.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 223.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 265.3 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 243.8 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 243.8 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 243.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 243.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 149.0 |
BN (mp-984) | <1 1 1> | <1 1 0> | 242.8 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 287.6 |
Al (mp-134) | <1 1 1> | <0 1 0> | 287.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 223.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 265.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 331.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 230.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 265.3 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 230.7 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 242.8 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 223.5 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 223.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 331.6 |
C (mp-66) | <1 1 0> | <0 1 0> | 287.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 331.6 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 74.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 74.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 74.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 -1> | 251.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 -1> | 243.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 287.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 331.6 |
SiC (mp-11714) | <1 0 0> | <1 0 -1> | 243.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 331.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 331.6 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 243.8 |
Au (mp-81) | <1 1 1> | <1 0 -1> | 243.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 265.3 |
C (mp-48) | <1 0 0> | <1 1 -1> | 251.3 |
C (mp-48) | <1 1 1> | <1 0 0> | 298.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi6P2O15 (mp-767410) | 0.6141 | 0.069 | 3 |
V2Bi4O11 (mp-743557) | 0.5651 | 0.100 | 3 |
Hg9(AsO4)4 (mp-541164) | 0.6126 | 0.013 | 3 |
Ca5Ge3O11 (mp-774105) | 0.5883 | 0.016 | 3 |
Cd3(PO4)2 (mp-27600) | 0.4934 | 0.020 | 3 |
SrFe2(PO4)2 (mp-607038) | 0.0357 | 0.000 | 4 |
NaV2Bi3O10 (mp-566700) | 0.4961 | 0.007 | 4 |
SrNi2(PO4)2 (mp-19647) | 0.5801 | 0.003 | 4 |
NaCd4(PO4)3 (mp-13718) | 0.5637 | 0.005 | 4 |
CaV2(PO4)2 (mvc-9882) | 0.5490 | 0.047 | 4 |
SrMgTi(PO4)2 (mvc-2641) | 0.5700 | 0.152 | 5 |
SrCaSn(PO4)2 (mvc-2825) | 0.5863 | 0.051 | 5 |
SrCaTi(PO4)2 (mvc-2770) | 0.5637 | 0.148 | 5 |
SrMgNi(PO4)2 (mvc-2996) | 0.5836 | 0.010 | 5 |
SrMgFe(PO4)2 (mvc-3019) | 0.5936 | 0.012 | 5 |
Na2LiCaVP2O9 (mp-763838) | 0.7210 | 0.114 | 6 |
Na2SrLiVP2O9 (mp-763837) | 0.7351 | 0.103 | 6 |
Na3Zn4P4H4NO16 (mp-772852) | 0.7120 | 0.005 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Sr_sv Fe_pv P O |
Final Energy/Atom-7.1869 eV |
Corrected Energy-418.0560 eV
-418.0560 eV = -373.7187 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)