Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.240 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.341 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 142.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 162.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 244.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 244.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 142.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 244.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 244.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 244.1 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 179.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 244.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 162.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 244.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 244.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 244.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 162.8 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 179.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 244.1 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 162.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 244.1 |
Au (mp-81) | <1 1 0> | <0 0 1> | 244.1 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 246.6 |
TiO2 (mp-390) | <1 0 0> | <1 0 -1> | 147.7 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 162.8 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 244.1 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 81.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V4Cr2O13 (mp-851269) | 0.2091 | 0.007 | 3 |
Li2Cr4O13 (mp-772323) | 0.4808 | 0.021 | 3 |
Li2Cr4O13 (mp-770390) | 0.3574 | 0.020 | 3 |
Cr2P4O13 (mp-562181) | 0.4221 | 0.011 | 3 |
Cr4P7O24 (mp-585323) | 0.4653 | 0.020 | 3 |
LiV3(CoO6)2 (mp-764446) | 0.4817 | 0.095 | 4 |
NaFe2(MoO4)3 (mp-567233) | 0.3805 | 0.002 | 4 |
Fe2Ag(MoO4)3 (mp-565482) | 0.3743 | 0.030 | 4 |
LiV(PO4)2 (mp-32471) | 0.4189 | 0.064 | 4 |
LiMn2(PO4)3 (mp-776889) | 0.4412 | 0.021 | 4 |
Li9Nb10Cr6(PO4)24 (mp-851292) | 0.6199 | 0.037 | 5 |
Li3Ti3Fe(PO4)6 (mp-743728) | 0.5831 | 0.017 | 5 |
LiNbSn3(PO4)6 (mp-759486) | 0.6095 | 0.017 | 5 |
LiMnV(PO4)3 (mp-770143) | 0.5766 | 0.036 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.6261 | 0.041 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6902 | 0.255 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.7206 | 0.011 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: V_pv Fe_pv O |
Final Energy/Atom-7.3068 eV |
Corrected Energy-640.6112 eV