Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.446 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa11Al14O32 + CaAl4O7 |
Band Gap4.981 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 155.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 195.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 263.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 42.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 64.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 93.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 312.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 106.8 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 248.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 263.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 108.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 320.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 64.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 217.1 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 312.2 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 263.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 64.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 93.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 285.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 117.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 297.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 64.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 112.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 285.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 108.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 271.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 135.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 274.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 216.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 85.4 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 135.4 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 62.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 162.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 213.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 216.6 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 1 -1> | 250.0 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 277.7 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 235.0 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 93.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 108.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 85.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 150.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 285.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 342.0 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 190.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 149.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 213.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 85.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 149.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
283 | 100 | 23 | 0 | -10 | 0 |
100 | 239 | 82 | 0 | -4 | 0 |
23 | 82 | 377 | 0 | -21 | 0 |
0 | 0 | 0 | 121 | 0 | -2 |
-10 | -4 | -21 | 0 | 47 | 0 |
0 | 0 | 0 | -2 | 0 | 78 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.2 | -1.8 | 0.2 | 0 | 0.8 | 0 |
-1.8 | 5.3 | -1.1 | 0 | -0.5 | 0 |
0.2 | -1.1 | 3.0 | 0 | 1.3 | 0 |
0 | 0 | 0 | 8.3 | 0 | 0.2 |
0.8 | -0.5 | 1.3 | 0 | 21.9 | 0 |
0 | 0 | 0 | 0.2 | 0 | 12.8 |
Shear Modulus GV96 GPa |
Bulk Modulus KV145 GPa |
Shear Modulus GR79 GPa |
Bulk Modulus KR142 GPa |
Shear Modulus GVRH87 GPa |
Bulk Modulus KVRH144 GPa |
Elastic Anisotropy1.06 |
Poisson's Ratio0.25 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Al O |
Final Energy/Atom-7.2283 eV |
Corrected Energy-106.8150 eV
-106.8150 eV = -101.1967 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)