Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2Si2O7 + YClO |
Band Gap4.565 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 302.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 216.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 216.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 120.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 111.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 302.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 172.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 120.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 302.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 172.8 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 111.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 345.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 302.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 111.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 302.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 247.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 167.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 259.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 345.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 86.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 43.2 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 223.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 129.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 43.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 223.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 216.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 216.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 216.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 259.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 345.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 129.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 302.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 345.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 302.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 345.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 167.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 302.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 216.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 129.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 345.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 345.6 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 172.8 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 302.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 216.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 302.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 345.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 216.0 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 223.8 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 111.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 239.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaPS3 (mp-9789) | 0.5370 | 0.000 | 3 |
PPbSe3 (mp-20316) | 0.5489 | 0.000 | 3 |
EuPSe3 (mp-20742) | 0.5455 | 0.000 | 3 |
BiAsO4 (mp-27911) | 0.5475 | 0.000 | 3 |
CaPSe3 (mp-11007) | 0.5026 | 0.000 | 3 |
Sm3Si2ClO8 (mp-23622) | 0.1046 | 0.000 | 4 |
Sm2SiTeO4 (mp-17812) | 0.5284 | 0.007 | 4 |
Nd3Si2ClO8 (mp-559764) | 0.1408 | 0.000 | 4 |
Yb3Si2ClO8 (mp-613785) | 0.2268 | 0.078 | 4 |
NaEr(PS3)2 (mp-12384) | 0.5235 | 0.000 | 4 |
Ga2I3 (mp-636675) | 0.7091 | 0.000 | 2 |
TlBr2 (mp-27398) | 0.7346 | 0.000 | 2 |
InI2 (mp-29312) | 0.7056 | 0.000 | 2 |
GaBr2 (mp-650841) | 0.7483 | 0.011 | 2 |
GaCl2 (mp-568848) | 0.7446 | 0.000 | 2 |
Na2YMoPO8 (mp-567058) | 0.6612 | 0.004 | 5 |
Na2YbMoPO8 (mp-579927) | 0.6589 | 0.056 | 5 |
K2YbMoPO8 (mp-565817) | 0.6600 | 0.000 | 5 |
YbZr7Si7PO32 (mp-690946) | 0.6512 | 0.018 | 5 |
ErZr11Si11PO48 (mp-690951) | 0.6606 | 0.008 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Si Cl O |
Final Energy/Atom-8.3211 eV |
Corrected Energy-488.4537 eV
-488.4537 eV = -465.9804 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)