Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.355 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH2O |
Band Gap5.456 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 293.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 197.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 260.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 260.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 67.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 225.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 131.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 260.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 271.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 295.4 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 246.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 92.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 130.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 325.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 300.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 130.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 225.9 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 231.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 260.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 65.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 67.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 325.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 246.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 323.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 32.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 231.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 32.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 46.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 325.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 231.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 225.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 227.9 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 262.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 260.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 262.6 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 184.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 46.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 260.4 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 225.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 260.4 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 231.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 164.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 67.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 97.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 231.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 195.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 229.8 |
BN (mp-984) | <0 0 1> | <1 0 1> | 225.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 260.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 162.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H5N2F (mp-27235) | 0.7463 | 0.147 | 3 |
H2CO (mp-625082) | 0.7407 | 0.314 | 3 |
HClO4 (mp-706301) | 0.7183 | 0.019 | 3 |
SnH4(ClO)2 (mp-721686) | 0.6532 | 0.006 | 4 |
HgH2NCl (mp-643754) | 0.7379 | 0.101 | 4 |
H3SNO3 (mp-757595) | 0.7291 | 0.078 | 4 |
H2O (mp-696735) | 0.2345 | 0.019 | 2 |
H2O (mp-24043) | 0.2630 | 0.025 | 2 |
H2O (mp-557082) | 0.1431 | 0.034 | 2 |
H2O (mp-558226) | 0.1577 | 0.033 | 2 |
H2O (mp-697111) | 0.4772 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H O |
Final Energy/Atom-4.9295 eV |
Corrected Energy-185.8912 eV
-185.8912 eV = -177.4638 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)