material

CuCSN

ID:

mp-559044

DOI:

10.17188/1270619


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.106 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.157 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CuS + N2 + C
Band Gap
2.124 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 32578 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.000 38.3
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.000 38.3
BN (mp-984) <0 0 1> <0 0 1> 0.000 38.3
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.000 126.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.002 114.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.002 114.9
LaF3 (mp-905) <0 0 1> <0 0 1> 0.002 319.3
BN (mp-984) <1 0 1> <0 0 1> 0.003 140.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.003 204.3
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.008 114.9
Ga2O3 (mp-886) <1 1 0> <1 0 1> 0.008 219.8
Ag (mp-124) <1 1 1> <0 0 1> 0.008 89.4
GaSe (mp-1943) <1 0 0> <0 0 1> 0.009 204.3
ZnSe (mp-1190) <1 0 0> <1 0 1> 0.010 131.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.011 51.1
Mg (mp-153) <0 0 1> <0 0 1> 0.011 114.9
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.013 102.2
TiO2 (mp-390) <0 0 1> <0 0 1> 0.019 102.2
GaAs (mp-2534) <1 0 0> <1 0 1> 0.020 131.9
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.020 306.5
C (mp-66) <1 1 1> <0 0 1> 0.020 89.4
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.024 126.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.025 89.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.027 242.6
ZnO (mp-2133) <1 0 0> <0 0 1> 0.028 140.5
Au (mp-81) <1 1 1> <0 0 1> 0.029 89.4
GaSe (mp-1943) <0 0 1> <0 0 1> 0.030 12.8
Al (mp-134) <1 0 0> <1 0 1> 0.030 131.9
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.030 307.7
MgO (mp-1265) <1 0 0> <1 0 1> 0.032 219.8
AlN (mp-661) <1 0 1> <0 0 1> 0.034 306.5
ZnO (mp-2133) <1 1 0> <0 0 1> 0.035 332.0
InP (mp-20351) <1 1 1> <0 0 1> 0.038 242.6
GaN (mp-804) <0 0 1> <0 0 1> 0.039 114.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.041 51.1
Cu (mp-30) <1 1 1> <0 0 1> 0.041 89.4
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.042 319.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.042 89.4
PbSe (mp-2201) <1 1 1> <0 0 1> 0.043 204.3
NaCl (mp-22862) <1 1 1> <0 0 1> 0.043 166.0
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.044 168.2
Si (mp-149) <1 1 1> <0 0 1> 0.044 51.1
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.045 219.8
GaN (mp-804) <1 0 0> <0 0 1> 0.047 268.2
Ge (mp-32) <1 0 0> <1 0 1> 0.048 131.9
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.050 319.3
C (mp-48) <1 0 1> <0 0 1> 0.056 242.6
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.058 332.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.059 204.3
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.060 131.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
53 27 30 0 0 0
27 53 30 0 0 0
30 30 207 0 0 0
0 0 0 10 0 0
0 0 0 0 10 0
0 0 0 0 0 13
Compliance Tensor Sij (10-12Pa-1)
26.3 -12.4 -2 0 0 0
-12.4 26.3 -2 0 0 0
-2 -2 5.4 0 0 0
0 0 0 103.7 0 0
0 0 0 0 103.7 0
0 0 0 0 0 77.6
Shear Modulus GV
22 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
40 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
47 GPa
Elastic Anisotropy
3.65
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn(CN)2 (mp-35751) 0.5614 0.254 3
Zn(CN)2 (mp-5245) 0.5622 0.255 3
AlPO4 (mp-545974) 0.4983 0.011 3
Mg(CN)2 (mp-36940) 0.5467 0.380 3
ZnSO4 (mp-545756) 0.5372 0.038 3
LiB(CN)4 (mp-13590) 0.6046 0.336 4
CuB(CN)4 (mp-13589) 0.6033 0.351 4
CuCSN (mp-672285) 0.0202 0.157 4
CuCSN (mp-553972) 0.3888 0.170 4
LiCo(CO)4 (mp-18939) 0.5773 0.407 4
SiO2 (mp-7087) 0.6852 0.012 2
CrN2 (mp-1014373) 0.6901 0.342 2
Si3O (mp-32566) 0.5761 0.448 2
CeSe2 (mp-1080249) 0.6901 0.528 2
CrN2 (mp-1097738) 0.6563 0.339 2
C (mp-1095534) 0.5583 1.121 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv C S N
Final Energy/Atom
-6.2940 eV
Corrected Energy
-52.0799 eV
Uncorrected energy = -50.3519 eV Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV Corrected energy = -52.0799 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 32578
Submitted by
User remarks:
  • Copper(I) thiocyanate - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)