Final Magnetic Moment3.209 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.185 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2O + Rb2Ce(NO3)6 + CeO2 + CuO + RbNO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPn3 [201] |
HallP 2 2 3 1n |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 170.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 120.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 170.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 170.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 120.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 170.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 241.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 170.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 120.7 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 120.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 241.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 1 0> | 170.7 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 120.7 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 170.7 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 170.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 120.7 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 170.7 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 120.7 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 120.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 120.7 |
Si (mp-149) | <1 1 0> | <1 1 0> | 170.7 |
YAlO3 (mp-3792) | <0 0 1> | <1 1 0> | 170.7 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 120.7 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 120.7 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 241.4 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 170.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3Co(NO2)6 (mp-24871) | 0.4016 | 0.049 | 4 |
Na3Co(NO2)6 (mp-19310) | 0.7372 | 0.064 | 4 |
YTl5Cu2(NO2)12 (mp-21963) | 0.1062 | 0.176 | 5 |
CeTl5Ni2(NO2)12 (mp-705086) | 0.0801 | 0.165 | 5 |
YTl5Cu2(NO2)12 (mp-562308) | 0.1118 | 0.176 | 5 |
CeTl5Ni2(NO2)12 (mp-565250) | 0.0808 | 0.165 | 5 |
CeTl5Cu2(NO2)12 (mp-555459) | 0.0311 | 0.177 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ce Cu_pv N O |
Final Energy/Atom-6.0865 eV |
Corrected Energy-568.5885 eV
Uncorrected energy = -535.6125 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Corrected energy = -568.5885 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)