Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.290 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.704 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 1 0> | <1 0 0> | 176.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 199.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 257.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 199.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 176.2 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 199.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 257.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 257.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 199.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 257.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 176.2 |
C (mp-48) | <1 0 1> | <0 1 0> | 257.0 |
TiO2 (mp-390) | <1 0 0> | <0 1 0> | 257.0 |
TiO2 (mp-390) | <1 0 1> | <1 0 -1> | 199.3 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 -1> | 199.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyPS4 (mp-5241) | 0.6166 | 0.000 | 3 |
ErPS4 (mp-5036) | 0.6090 | 0.000 | 3 |
HoPS4 (mp-18532) | 0.6128 | 0.000 | 3 |
YbPS4 (mp-555732) | 0.6146 | 0.074 | 3 |
TbPS4 (mp-4672) | 0.6204 | 0.000 | 3 |
K3Dy(AsS4)2 (mp-866661) | 0.1250 | 0.000 | 4 |
K3Gd3(PS4)4 (mp-604889) | 0.5825 | 0.000 | 4 |
K3Nd3(PS4)4 (mp-555172) | 0.5922 | 0.000 | 4 |
K3Sm(AsS4)2 (mp-560964) | 0.0536 | 0.000 | 4 |
NaNdSiO4 (mp-13774) | 0.6401 | 0.000 | 4 |
TlBr2 (mp-27398) | 0.6441 | 0.000 | 2 |
InI2 (mp-29312) | 0.6120 | 0.000 | 2 |
InBr2 (mp-568108) | 0.7035 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.7080 | 0.000 | 2 |
KF5 (mp-1095521) | 0.7454 | 0.053 | 2 |
SrLaTl(AsO4)2 (mp-685195) | 0.6665 | 0.000 | 5 |
K2HoPWO8 (mp-565678) | 0.6948 | 0.000 | 5 |
K2YbMoPO8 (mp-565817) | 0.7308 | 0.003 | 5 |
K2BiMoPO8 (mp-566924) | 0.6857 | 0.000 | 5 |
K2BiPWO8 (mp-566769) | 0.6852 | 0.001 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Nd_3 As S |
Final Energy/Atom-4.5182 eV |
Corrected Energy-134.5586 eV
Uncorrected energy = -126.5106 eV
Composition-based energy adjustment (-0.503 eV/atom x 16.0 atoms) = -8.0480 eV
Corrected energy = -134.5586 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)