Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.988 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + KCuPO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 147.0 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 268.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 201.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 217.0 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 268.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 290.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 298.6 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 289.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 223.6 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 268.5 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 216.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 268.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 201.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 290.7 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 268.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 208.9 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 217.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 217.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 -1> | 72.3 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 288.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 223.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 207.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 238.9 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 144.7 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 268.5 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 289.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 298.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 288.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 201.3 |
BN (mp-984) | <0 0 1> | <1 0 1> | 223.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 134.2 |
BN (mp-984) | <1 1 1> | <1 -1 0> | 268.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 223.6 |
MoS2 (mp-1434) | <0 0 1> | <1 1 -1> | 185.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 289.3 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 298.6 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 223.6 |
TiO2 (mp-2657) | <1 0 0> | <1 -1 0> | 179.0 |
C (mp-66) | <1 1 1> | <0 1 -1> | 217.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 223.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 -1> | 278.8 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 208.9 |
Mg (mp-153) | <1 1 1> | <0 1 -1> | 217.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 288.4 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 288.4 |
TeO2 (mp-2125) | <0 1 1> | <1 1 1> | 147.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 238.9 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 216.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 223.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 298.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3(PO4)4 (mp-31797) | 0.4661 | 0.049 | 4 |
LiMnP2O7 (mp-540242) | 0.5701 | 0.021 | 4 |
LiCr4(PO4)3 (mp-540459) | 0.5582 | 0.028 | 4 |
LiCu4(PO4)3 (mp-673145) | 0.4198 | 0.056 | 4 |
Li3Sn3(PO4)4 (mp-758291) | 0.5641 | 0.098 | 4 |
CrN2 (mp-1016069) | 0.7036 | 0.445 | 2 |
Cu2PO4 (mp-17281) | 0.5221 | 0.000 | 3 |
Cr4(PO4)3 (mp-540460) | 0.5645 | 0.040 | 3 |
V2Cu2O7 (mp-559660) | 0.5562 | 0.000 | 3 |
Cu4(PO4)3 (mp-673151) | 0.4132 | 0.026 | 3 |
Li2Cr2O7 (mp-772297) | 0.5783 | 0.068 | 3 |
Na8Al11Si13(AgO16)3 (mp-677572) | 0.6973 | 0.118 | 5 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.7252 | 0.005 | 5 |
V3H8C2NO7 (mp-600369) | 0.6479 | 0.172 | 5 |
V3H6CNO7 (mp-600514) | 0.5957 | 0.150 | 5 |
Ga2P3H12(NO4)3 (mp-758916) | 0.6246 | 0.004 | 5 |
Mo12PH24C6N3O40 (mp-600535) | 0.7256 | 0.199 | 6 |
SiMo12H24C6N3O40 (mp-744841) | 0.7412 | 0.235 | 6 |
Mo12PH24C6N3O40 (mp-745080) | 0.7147 | 0.199 | 6 |
K3Ca2Mg10Si16(HO12)4 (mp-720217) | 0.7341 | 0.500 | 6 |
NaCaMgAl(SiO3)4 (mp-720244) | 0.6443 | 0.394 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points32 |
U Values-- |
PseudopotentialsVASP PAW: K_sv Cu_pv P O |
Final Energy/Atom-6.2135 eV |
Corrected Energy-265.3962 eV
-265.3962 eV = -248.5413 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)