Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-3.026 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.096 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 84.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 119.9 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 254.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 84.8 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 119.9 |
Si (mp-149) | <1 1 1> | <1 0 0> | 254.4 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 169.6 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 239.8 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 119.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 254.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 119.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 254.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 239.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 254.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 84.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 119.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 169.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 84.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 254.4 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 254.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 84.8 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 119.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 239.8 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 254.4 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 254.4 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 84.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 119.9 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 239.8 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 254.4 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 169.6 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 169.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs2KCrF6 (mp-560956) | 0.0095 | 0.000 | 4 |
Cs2AsBrCl6 (mp-989511) | 0.0043 | 0.007 | 4 |
CsRb2InF6 (mp-989595) | 0.0053 | 0.026 | 4 |
KRb2GaF6 (mp-13190) | 0.0143 | 0.000 | 4 |
Cs2NaNF6 (mp-989527) | 0.0046 | 0.000 | 4 |
La2O3 (mp-33032) | 0.5161 | 0.889 | 2 |
Mn4N (mp-637576) | 0.5104 | 1.993 | 2 |
Ni4N (mp-20839) | 0.5161 | 2.016 | 2 |
Ca3N2 (mp-1013524) | 0.5161 | 0.511 | 2 |
Sr3N2 (mp-1013529) | 0.5161 | 0.557 | 2 |
Li6Br3N (mp-27508) | 0.0309 | 0.064 | 3 |
K3ReH6 (mp-690789) | 0.1195 | 0.183 | 3 |
TiTl3F6 (mp-15635) | 0.0713 | 0.097 | 3 |
TbCs3F6 (mp-696965) | 0.0634 | 0.000 | 3 |
Ba3WO6 (mp-25172) | 0.1198 | 0.054 | 3 |
BaLiPrTeO6 (mp-41219) | 0.4249 | 0.020 | 5 |
K3Ba2Pr2(BiO5)3 (mp-686204) | 0.4256 | 0.051 | 5 |
Ba20Y10Cu(Ru3O20)3 (mp-686442) | 0.4123 | 0.005 | 5 |
BaLiLaTeO6 (mp-40189) | 0.4181 | 0.005 | 5 |
BaSrLaBiO6 (mp-40802) | 0.3799 | 0.248 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.7244 | 0.059 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points28 |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: F K_sv Fe_pv Cs_sv |
Final Energy/Atom-4.7320 eV |
Corrected Energy-50.0530 eV
-50.0530 eV = -47.3200 eV (uncorrected energy) - 2.7330 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)