Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiBi2O5 + TiO2 |
Band Gap2.624 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 1 1> | 187.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 216.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 108.4 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 187.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 216.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 216.9 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 153.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 108.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 108.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 153.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 187.8 |
C (mp-66) | <1 0 0> | <1 1 0> | 153.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 108.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 216.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 153.3 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 187.8 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 153.3 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 187.8 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 216.9 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 108.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 108.4 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 108.4 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 153.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 187.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 153.3 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 108.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 108.4 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 216.9 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 108.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc2Si2O7 (mp-7640) | 0.0178 | 0.085 | 3 |
Yb2Ti2O7 (mp-22431) | 0.0487 | 0.172 | 3 |
Nd2Ti2O7 (mp-555785) | 0.0454 | 0.040 | 3 |
Eu2Ti2O7 (mp-505801) | 0.0386 | 0.000 | 3 |
La2Ti2O7 (mp-4423) | 0.0343 | 0.050 | 3 |
Mn2Hg2SF6 (mp-600275) | 0.0501 | 0.000 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.0596 | 0.000 | 4 |
Mn2Hg2SF6 (mp-556900) | 0.0688 | 0.000 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.0313 | 0.000 | 4 |
Ni2Hg2SF6 (mp-559259) | 0.1609 | 0.000 | 4 |
LiCaTa2O6F (mp-39511) | 0.2251 | 0.030 | 5 |
YbTi2CdO6F (mp-677010) | 0.1882 | 0.121 | 5 |
Ca2Nd2Nb3FeO14 (mvc-16570) | 0.2524 | 0.029 | 5 |
EuTi2CdO6F (mp-684730) | 0.1761 | 0.359 | 5 |
Ca2Nd2Nb3FeO14 (mp-40206) | 0.2068 | 0.029 | 5 |
NaYbTiNbO6F (mp-684861) | 0.3897 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.4617 | 0.035 | 6 |
NaEuTiNbO6F (mp-43048) | 0.3451 | 0.019 | 6 |
NaCeTiNbO6F (mp-43055) | 0.4401 | 0.028 | 6 |
NaNdTiNbO6F (mp-43134) | 0.4599 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Bi O |
Final Energy/Atom-7.4893 eV |
Corrected Energy-174.5974 eV
-174.5974 eV = -164.7654 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)