Final Magnetic Moment1.323 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.812 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.224 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYbF2 + GeO2 + YbGeO3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 232.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 232.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 166.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 166.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 216.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 232.9 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 183.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 166.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 166.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 155.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 216.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 133.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 108.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 232.9 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 198.5 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 108.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 155.3 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 232.9 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 133.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 108.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 216.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 310.6 |
BN (mp-984) | <1 1 0> | <1 0 1> | 198.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 310.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 216.2 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 232.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 166.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 198.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 183.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 166.5 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 166.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 216.2 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 166.5 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 1 0> | 232.9 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 166.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 77.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 108.1 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 232.9 |
Mg (mp-153) | <1 1 1> | <0 1 1> | 183.7 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 266.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 77.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 77.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 108.1 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 232.9 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 232.9 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 108.1 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 216.2 |
ZnO (mp-2133) | <1 1 0> | <0 1 1> | 183.7 |
GaP (mp-2490) | <1 0 0> | <0 1 1> | 183.7 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 166.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2Cr2As2O9 (mp-622624) | 0.7451 | 0.000 | 4 |
Rb3U2Ge2O11 (mp-558697) | 0.6487 | 0.000 | 4 |
K2Ni(MoO4)2 (mp-565389) | 0.6990 | 0.002 | 4 |
K8Hf(MoO4)6 (mp-566452) | 0.7489 | 0.000 | 4 |
CaCoP2O7 (mp-18776) | 0.7492 | 0.008 | 4 |
Na3Ca2Fe5(SiO3)10 (mp-735984) | 0.7109 | 0.146 | 5 |
K3Fe3P4H2O17 (mp-745015) | 0.7123 | 0.000 | 5 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6578 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Ge_d O F |
Final Energy/Atom-5.8458 eV |
Corrected Energy-275.1231 eV
Uncorrected energy = -257.2131 eV
Composition-based energy adjustment (-0.687 eV/atom x 18.0 atoms) = -12.3660 eV
Composition-based energy adjustment (-0.462 eV/atom x 12.0 atoms) = -5.5440 eV
Corrected energy = -275.1231 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)