Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.092 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.112 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKSO2F + CO2 + CF4 |
Band Gap5.265 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 200.2 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 165.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 200.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 151.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 259.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 66.7 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 259.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 266.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 165.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 266.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 266.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 271.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 175.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 165.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 66.7 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 90.3 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 165.1 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 129.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 200.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 200.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 266.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 266.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 266.9 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 175.6 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 151.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 266.9 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 266.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 179.1 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 259.1 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 66.7 |
SiC (mp-11714) | <1 0 1> | <1 0 1> | 129.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 179.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 200.2 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 266.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 266.9 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 89.6 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 259.1 |
Au (mp-81) | <1 0 0> | <1 0 1> | 259.1 |
Au (mp-81) | <1 1 0> | <0 0 1> | 200.2 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 266.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 266.9 |
WS2 (mp-224) | <0 0 1> | <1 1 0> | 175.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 200.2 |
C (mp-48) | <1 0 0> | <1 0 0> | 268.7 |
C (mp-48) | <1 0 1> | <1 0 1> | 259.1 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 1> | 165.1 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 200.2 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 268.7 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 133.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb4CO4 (mp-556527) | 0.7281 | 0.196 | 3 |
SiH17S3N5 (mp-557080) | 0.7428 | 0.000 | 4 |
HgH3CSO3 (mp-738615) | 0.7123 | 0.230 | 5 |
H24C8Se(NO2)2 (mp-677203) | 0.7196 | 0.221 | 5 |
RbCS(OF)3 (mp-672209) | 0.5858 | 0.120 | 5 |
HgCS(OF)3 (mp-560125) | 0.6109 | 0.159 | 5 |
H24C8S(NO2)2 (mp-695436) | 0.6240 | 0.145 | 5 |
VH24C8S2N2O9 (mp-745144) | 0.7067 | 0.185 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv C S O F |
Final Energy/Atom-5.5153 eV |
Corrected Energy-321.5287 eV
Uncorrected energy = -297.8287 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Composition-based energy adjustment (-0.687 eV/atom x 18.0 atoms) = -12.3660 eV
Composition-based energy adjustment (-0.462 eV/atom x 18.0 atoms) = -8.3160 eV
Corrected energy = -321.5287 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)