Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.797 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.561 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <1 1 1> | <0 1 0> | 136.9 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 227.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 227.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 113.7 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 227.4 |
C (mp-48) | <1 1 1> | <0 1 0> | 136.9 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 227.4 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 113.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Lu(PO3)3 (mp-557585) | 0.2520 | 0.004 | 3 |
Y(PO3)3 (mp-554423) | 0.2563 | 0.000 | 3 |
Yb(PO3)3 (mp-583593) | 0.2760 | 0.000 | 3 |
Y(PO3)3 (mp-1020797) | 0.2579 | 0.010 | 3 |
MoP2O7 (mp-32085) | 0.2777 | 0.006 | 3 |
ZrFe(PO4)3 (mp-769438) | 0.3665 | 0.083 | 4 |
Sb3P6WO24 (mp-775210) | 0.3020 | 0.033 | 4 |
LiP5W3O19 (mp-763535) | 0.3954 | 0.099 | 4 |
Mn7Sn(PO4)12 (mp-778765) | 0.3932 | 0.070 | 4 |
Nb2Co(P2O7)3 (mp-652471) | 0.3662 | 0.012 | 4 |
Cr5O12 (mp-773920) | 0.5938 | 0.000 | 2 |
Mo9O25 (mp-565530) | 0.7155 | 0.009 | 2 |
Mo4O11 (mp-565865) | 0.6838 | 0.026 | 2 |
V5O12 (mp-778252) | 0.5840 | 0.024 | 2 |
Cr3O8 (mp-557959) | 0.6462 | 0.048 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.5670 | 0.041 | 5 |
MgCr3Se2(SO6)4 (mp-769544) | 0.4826 | 0.373 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.5411 | 0.002 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.4693 | 0.455 | 5 |
Ti6In2Si2P12O49 (mp-560564) | 0.5782 | 0.000 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.7167 | 0.009 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.7072 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6966 | 0.014 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Cd P O |
Final Energy/Atom-7.6728 eV |
Corrected Energy-979.7287 eV
-979.7287 eV = -920.7363 eV (uncorrected energy) - 58.9924 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)