Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.751 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbAlF4 + RbF3 + TbF3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 211.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 264.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 211.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 211.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 172.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 158.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 211.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 211.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 225.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 317.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 172.7 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 225.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 211.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 172.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 211.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 211.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 211.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 52.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 211.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 211.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 99.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 211.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 264.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 158.5 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 211.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 158.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 211.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 211.3 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 225.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 317.0 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 299.1 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 264.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 211.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 264.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 99.7 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 1> | 225.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 317.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 199.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 158.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 211.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 225.7 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 317.0 |
Si (mp-149) | <1 1 0> | <0 0 1> | 211.3 |
Si (mp-149) | <1 1 1> | <0 0 1> | 52.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 211.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 211.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 211.3 |
C (mp-48) | <1 1 0> | <1 0 0> | 99.7 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 299.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points8 |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Rb_sv Al F |
Final Energy/Atom-5.6728 eV |
Corrected Energy-249.6042 eV
-249.6042 eV = -249.6042 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)