Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.936 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.650 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 189.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 149.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 207.7 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 149.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 -1> | 155.7 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 189.2 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 207.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 149.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 149.8 |
WS2 (mp-224) | <1 1 0> | <1 0 -1> | 155.7 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 207.7 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 158.1 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 103.8 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 182.2 |
GaTe (mp-542812) | <0 1 0> | <1 1 0> | 182.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2Ge2O5 (mp-771185) | 0.5872 | 0.008 | 3 |
Tb2Si2O7 (mp-17308) | 0.5876 | 0.000 | 3 |
Tm2Si2O7 (mp-18318) | 0.5833 | 0.037 | 3 |
Ho2Si2O7 (mp-16809) | 0.5796 | 0.012 | 3 |
Dy2Si2O7 (mp-17062) | 0.5840 | 0.005 | 3 |
Li7Fe2P7O24 (mp-761522) | 0.6042 | 0.069 | 4 |
Li7Sb2P7O24 (mp-762329) | 0.5837 | 0.073 | 4 |
Na3B(PO4)2 (mp-559783) | 0.5312 | 0.000 | 4 |
LiBiP2O7 (mp-584134) | 0.6194 | 0.035 | 4 |
Na5B(SO4)4 (mp-1020599) | 0.4761 | 0.001 | 4 |
KCu3Ag(MoO4)4 (mp-699550) | 0.6975 | 0.019 | 5 |
KNaZnP2O7 (mp-554157) | 0.7333 | 0.000 | 5 |
BaNaNd(GeO3)3 (mp-14353) | 0.7465 | 0.006 | 5 |
LiAg2P3(HO5)2 (mp-695951) | 0.7440 | 0.020 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ca_sv Al P O |
Final Energy/Atom-6.6490 eV |
Corrected Energy-394.8159 eV
-394.8159 eV = -372.3426 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)