Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.887 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density15.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 289.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 1> | 246.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 151.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 108.5 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 197.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 206.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 151.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 108.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 123.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 123.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 246.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 334.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 331.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 68.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 344.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 68.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 108.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 234.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.2 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 141.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 200.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 316.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 165.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 82.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 200.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 141.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 123.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 197.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 283.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 289.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 247.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 108.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 289.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 55.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 137.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 72.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 197.0 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 246.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 167.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 234.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 178.9 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 246.3 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 141.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 220.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 283.8 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 283.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 325.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 344.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 344.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
132 | 89 | 74 | 0 | 0 | 0 |
89 | 132 | 74 | 0 | 0 | 0 |
74 | 74 | 196 | 0 | 0 | 0 |
0 | 0 | 0 | 37 | 0 | 0 |
0 | 0 | 0 | 0 | 37 | 0 |
0 | 0 | 0 | 0 | 0 | 72 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
14.8 | -8.7 | -2.3 | 0 | 0 | 0 |
-8.7 | 14.8 | -2.3 | 0 | 0 | 0 |
-2.3 | -2.3 | 6.8 | 0 | 0 | 0 |
0 | 0 | 0 | 27.1 | 0 | 0 |
0 | 0 | 0 | 0 | 27.1 | 0 |
0 | 0 | 0 | 0 | 0 | 13.9 |
Shear Modulus GV44 GPa |
Bulk Modulus KV104 GPa |
Shear Modulus GR37 GPa |
Bulk Modulus KR102 GPa |
Shear Modulus GVRH41 GPa |
Bulk Modulus KVRH103 GPa |
Elastic Anisotropy0.92 |
Poisson's Ratio0.33 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaSb2Au (mp-675224) | 0.1796 | 0.286 | 3 |
ErAu2 (mp-2466) | 0.0163 | 0.000 | 2 |
YAu2 (mp-1018113) | 0.0287 | 0.000 | 2 |
Si2Mo (mp-2592) | 0.0317 | 0.000 | 2 |
Si2W (mp-1620) | 0.0237 | 0.000 | 2 |
YbAu2 (mp-1668) | 0.0310 | 0.000 | 2 |
Si (mp-1056579) | 0.1991 | 0.486 | 1 |
Sc (mp-601273) | 0.2490 | 0.128 | 1 |
Pa (mp-62) | 0.0835 | 0.027 | 1 |
Pr (mp-1056311) | 0.4267 | 0.086 | 1 |
Sn (mp-55) | 0.3157 | 0.063 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Au |
Final Energy/Atom-4.5617 eV |
Corrected Energy-13.6850 eV
-13.6850 eV = -13.6850 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)