Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.491 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 265.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 265.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 298.3 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 312.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 158.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 298.3 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 329.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 264.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 264.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 282.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 198.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 235.4 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 329.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 141.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 234.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 265.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 264.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 298.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 141.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 187.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 312.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 211.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 264.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 264.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 312.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 264.3 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 62.4 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 235.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 211.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 329.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 232.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 99.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 265.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 211.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 211.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 264.3 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 312.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 364.6 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 212.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 298.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 212.4 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 283.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 52.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 187.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 211.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 235.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 211.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 232.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 158.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 133.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyCoSn (mp-22228) | 0.1840 | 0.000 | 3 |
TbCoSn (mp-646450) | 0.2004 | 0.000 | 3 |
DyGaCo (mp-605252) | 0.2036 | 0.000 | 3 |
ErCoSn (mp-11851) | 0.0555 | 0.000 | 3 |
GdGeRu (mp-19714) | 0.2453 | 0.000 | 3 |
EuIn2(GeIr)4 (mp-1095411) | 0.7221 | 0.000 | 4 |
EuZn2 (mp-681) | 0.6475 | 0.000 | 2 |
EuGa2 (mp-917274) | 0.6462 | 0.000 | 2 |
BaIn2 (mp-22141) | 0.6289 | 0.000 | 2 |
SrZn2 (mp-569426) | 0.6225 | 0.000 | 2 |
LaZn2 (mp-567258) | 0.6403 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Co Sn_d |
Final Energy/Atom-5.7241 eV |
Corrected Energy-68.6892 eV
-68.6892 eV = -68.6892 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)