Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.186 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.687 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42m [121] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 94.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 332.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 282.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 66.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 332.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 282.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 266.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 167.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 266.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 199.7 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 199.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 266.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 332.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 282.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 266.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 199.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 266.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 94.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 282.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 199.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 66.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 133.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 199.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 199.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 282.4 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 282.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 282.4 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 94.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 282.4 |
C (mp-66) | <1 0 0> | <1 1 0> | 282.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 332.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 266.2 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 282.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 199.7 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 66.6 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 199.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 266.2 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 332.8 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 0> | 266.2 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 199.7 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 94.1 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 199.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 332.8 |
Au (mp-81) | <1 1 1> | <1 0 0> | 266.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 282.4 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 180.6 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 199.7 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 199.7 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 133.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoSiO4 (mp-633897) | 0.5749 | 0.356 | 3 |
BeCrO4 (mp-770887) | 0.5033 | 0.011 | 3 |
NiPO4 (mp-705637) | 0.5457 | 0.537 | 3 |
PNO (mp-36779) | 0.5284 | 0.015 | 3 |
AlPO4 (mp-558088) | 0.5920 | 0.025 | 3 |
Rb2Al2Si3O10 (mp-975622) | 0.6369 | 0.009 | 4 |
CsSi3HO7 (mp-758180) | 0.6001 | 0.002 | 4 |
K2Be(Si2O5)2 (mp-557802) | 0.7108 | 0.000 | 4 |
KAlSi3O8 (mp-697670) | 0.7160 | 0.000 | 4 |
K2Al2Si3O10 (mp-1019744) | 0.6415 | 0.018 | 4 |
SiO2 (mp-556994) | 0.2595 | 0.083 | 2 |
SiO2 (mp-557873) | 0.3109 | 0.061 | 2 |
SiO2 (mp-558569) | 0.3108 | 0.073 | 2 |
SiO2 (mp-560152) | 0.2497 | 0.098 | 2 |
CeSe2 (mp-1080370) | 0.2421 | 0.503 | 2 |
RbB2P2HO9 (mp-758281) | 0.6343 | 0.000 | 5 |
RbZnB(PO4)2 (mp-557658) | 0.6946 | 0.000 | 5 |
CsZnB(PO4)2 (mp-560244) | 0.6854 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8245 eV |
Corrected Energy-199.0238 eV
-199.0238 eV = -187.7872 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)