Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.258 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.642 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 184.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 330.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 191.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 330.7 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 140.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 184.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 198.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 154.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 330.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 184.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 184.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 330.7 |
TePb (mp-19717) | <1 1 0> | <1 1 -1> | 184.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 264.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 140.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 198.4 |
Al (mp-134) | <1 1 0> | <1 1 -1> | 184.2 |
CdTe (mp-406) | <1 1 0> | <1 1 -1> | 184.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 140.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 330.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 264.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 330.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 -1> | 184.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 198.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 264.5 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 -1> | 184.2 |
InSb (mp-20012) | <1 1 0> | <1 1 -1> | 184.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 264.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 154.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 330.7 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 -1> | 184.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 330.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 264.5 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 264.5 |
MoSe2 (mp-1634) | <1 1 0> | <1 1 -1> | 184.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 330.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 154.3 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 264.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 330.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 330.7 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 330.7 |
NaCl (mp-22862) | <1 1 0> | <1 1 -1> | 184.2 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 330.7 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 198.4 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 264.5 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 264.5 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 154.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 198.4 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 264.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.4361 | 0.012 | 3 |
AlPO4 (mp-557362) | 0.4549 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.4158 | 0.011 | 3 |
Be(PO3)2 (mp-560521) | 0.3678 | 0.003 | 3 |
AlPO4 (mp-1019510) | 0.4242 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.6957 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.7204 | 0.002 | 4 |
CsAlSiO4 (mp-561457) | 0.7119 | 0.000 | 4 |
CsSi2HO5 (mp-557780) | 0.7049 | 0.005 | 4 |
CsBePO4 (mp-15395) | 0.6383 | 0.000 | 4 |
SiO2 (mp-600031) | 0.1920 | 0.011 | 2 |
SiO2 (mp-639506) | 0.1879 | 0.013 | 2 |
SiO2 (mp-560336) | 0.1660 | 0.013 | 2 |
CeSe2 (mp-1080854) | 0.0792 | 0.522 | 2 |
CeSe2 (mp-1099575) | 0.1895 | 0.522 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8958 eV |
Corrected Energy-451.6553 eV
-451.6553 eV = -426.3729 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)