Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.964 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.363 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 262.3 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 262.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 205.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 309.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 232.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 102.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 243.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 243.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 243.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 77.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 162.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 211.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 205.8 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 257.4 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 211.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 131.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 232.0 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 309.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 102.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 162.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 152.1 |
PbS (mp-21276) | <1 1 0> | <1 1 -1> | 262.3 |
C (mp-66) | <1 1 0> | <0 1 0> | 309.4 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 232.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 162.3 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 -1> | 211.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 243.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 102.9 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 243.5 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 105.9 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 1> | 152.1 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 309.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 309.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 243.5 |
C (mp-48) | <0 0 1> | <0 1 0> | 309.4 |
C (mp-48) | <1 1 1> | <0 1 0> | 232.0 |
WSe2 (mp-1821) | <1 0 0> | <1 0 1> | 152.1 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 102.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 154.7 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 162.3 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 232.0 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 309.4 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 232.0 |
ZnO (mp-2133) | <1 0 0> | <1 0 -1> | 105.9 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 309.4 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 0> | 257.4 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 162.3 |
ZnTe (mp-2176) | <1 1 0> | <1 1 -1> | 262.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pb3SO6 (mp-22023) | 0.6162 | 0.007 | 3 |
Pb3SO6 (mp-559143) | 0.6203 | 0.004 | 3 |
Hg9(PO4)4 (mp-542054) | 0.7340 | 0.014 | 3 |
Sn2SO5 (mp-28025) | 0.7259 | 0.058 | 3 |
Bi3(PO5)2 (mvc-15217) | 0.6563 | 0.074 | 3 |
Ba2VP2O11 (mp-863298) | 0.4797 | 0.187 | 4 |
Te2S(O2F3)2 (mp-555457) | 0.7140 | 0.000 | 4 |
Ba2TeP2O9 (mp-560742) | 0.6322 | 0.000 | 4 |
KCrIO6 (mp-566379) | 0.6866 | 0.002 | 4 |
Ba2VP2O9 (mp-566252) | 0.6551 | 0.000 | 4 |
BaVCdP2O9 (mp-699566) | 0.5288 | 0.006 | 5 |
Rb2Cu3H2S3O14 (mp-697969) | 0.6864 | 0.250 | 5 |
K2Sb2S(O2F3)2 (mp-557470) | 0.7038 | 0.000 | 5 |
AgH12C4S5N (mp-698405) | 0.7353 | 0.081 | 5 |
Tl3Hg2S3ClO12 (mp-554279) | 0.1654 | 0.000 | 5 |
VH24C8S2N2O9 (mp-745144) | 0.7423 | 0.185 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Hg S Cl O |
Final Energy/Atom-5.1150 eV |
Corrected Energy-234.3368 eV
Uncorrected energy = -214.8308 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -234.3368 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)