Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.374 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.724 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 228.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 242.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 242.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 228.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 107.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 188.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 228.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 320.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 320.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 159.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 274.3 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 137.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 188.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 188.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 274.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 323.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 318.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 274.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 137.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 242.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 182.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 212.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 274.3 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 228.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 274.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 274.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 242.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 215.6 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 91.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 142.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 137.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 142.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 228.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 242.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 274.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 318.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 350.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 242.5 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 296.4 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 242.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 212.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 53.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 269.5 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 91.4 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 265.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 134.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 350.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 296.4 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 161.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 274.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaFeO3 (mp-868578) | 0.5870 | 0.037 | 3 |
Ga7(Fe3O8)3 (mp-767269) | 0.5700 | 0.040 | 3 |
AlGaO3 (mp-772187) | 0.6156 | 0.029 | 3 |
GaFeO3 (mp-649086) | 0.5969 | 0.524 | 3 |
KAl9O14 (mp-1019803) | 0.5230 | 0.010 | 3 |
LiCoOF2 (mp-780318) | 0.7292 | 0.223 | 4 |
LiFeOF2 (mp-780152) | 0.7262 | 0.512 | 4 |
NaTi2Ga5O12 (mp-554441) | 0.1552 | 0.001 | 4 |
Zn4Co5(TeO6)3 (mvc-3070) | 0.7274 | 0.206 | 4 |
Zn4Cu5(TeO6)3 (mp-557936) | 0.7101 | 0.019 | 4 |
Sc2O3 (mp-775837) | 0.6617 | 0.082 | 2 |
Fe2O3 (mp-628327) | 0.7237 | 0.749 | 2 |
Al2O3 (mp-2254) | 0.5941 | 0.017 | 2 |
Fe2O3 (mp-715516) | 0.6285 | 0.749 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ti_pv Al O |
Final Energy/Atom-7.7131 eV |
Corrected Energy-325.0107 eV
Uncorrected energy = -308.5227 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -325.0107 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)