Final Magnetic Moment3.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.517 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr2CoMoO6 |
Band Gap0.619 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 150.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 218.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 150.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 137.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 240.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 300.3 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 54.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 228.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 129.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 137.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 193.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 228.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 150.2 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 284.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 228.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 54.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 240.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 90.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 54.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 182.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 150.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 193.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 228.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 150.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 273.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 228.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 284.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 330.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 270.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.3 |
Te2Mo (mp-602) | <1 1 0> | <1 1 1> | 284.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 137.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 150.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 60.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 240.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 213.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 90.1 |
MoS2 (mp-1434) | <1 1 1> | <1 0 0> | 228.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 330.4 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 218.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 137.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 150.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 300.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 150.2 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 240.3 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 163.9 |
SiC (mp-7631) | <1 1 1> | <1 0 1> | 163.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 150.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 270.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KCuF3 (mp-1079287) | 0.2808 | 0.000 | 3 |
KCrF3 (mp-560547) | 0.2891 | 0.005 | 3 |
MnNF3 (mp-1078939) | 0.3113 | 1.042 | 3 |
KCuF3 (mp-1080828) | 0.2888 | 0.001 | 3 |
KCuF3 (mp-669347) | 0.2505 | 0.000 | 3 |
La8Al7BO24 (mp-997588) | 0.3074 | 0.119 | 4 |
Ba32Sb7Pb25O96 (mp-686499) | 0.2816 | 0.000 | 4 |
Ba2CoMoO6 (mp-561894) | 0.2165 | 0.009 | 4 |
K2NaMnF6 (mp-1079339) | 0.2968 | 0.000 | 4 |
Sr2MnSbO6 (mp-557296) | 0.1182 | 0.020 | 4 |
Mn4N (mp-637576) | 0.4600 | 1.987 | 2 |
Fe2O3 (mp-1068212) | 0.4654 | 0.860 | 2 |
Fe4P (mp-20885) | 0.4775 | 0.686 | 2 |
Ni4O (mp-1094082) | 0.4791 | 1.616 | 2 |
Ni4N (mp-1094090) | 0.4791 | 0.067 | 2 |
K4Na4Mo3W5O24 (mp-1099601) | 0.2697 | 0.012 | 5 |
Sr2Ca2Fe(CoO4)3 (mp-1099605) | 0.2677 | 0.233 | 5 |
Sr5Ca3Fe2(CoO4)6 (mp-1076260) | 0.2666 | 0.228 | 5 |
Ba2Sr6Co5(CuO8)3 (mp-1076429) | 0.2489 | 0.175 | 5 |
Sr4Ca4Fe3Co5O24 (mp-1076674) | 0.2613 | 0.037 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.5326 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVMo: 4.38 eV |
PseudopotentialsVASP PAW: Sr_sv Co Mo_pv O |
Final Energy/Atom-6.6568 eV |
Corrected Energy-76.1864 eV
-76.1864 eV = -66.5676 eV (uncorrected energy) - 5.4050 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)