Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-2.759 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.798 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 210.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 316.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 316.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 263.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 316.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 263.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 158.2 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 210.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 210.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 210.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 210.9 |
Si (mp-149) | <1 1 0> | <0 0 1> | 210.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 316.4 |
C (mp-48) | <1 0 0> | <0 0 1> | 210.9 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 105.5 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 316.4 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 263.7 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 158.2 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 263.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 263.7 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 198.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 263.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 210.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 263.7 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 210.9 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 263.7 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 210.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 263.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 158.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 263.7 |
CsI (mp-614603) | <1 1 0> | <0 0 1> | 263.7 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 263.7 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 210.9 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 158.2 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 210.9 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 263.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2ZrSi2O7 (mp-559489) | 0.6404 | 0.000 | 4 |
Cs2UP2O9 (mp-561356) | 0.6417 | 0.000 | 4 |
K4V3S5O23 (mp-579382) | 0.5073 | 0.017 | 4 |
Ba3Nb2(P2O9)2 (mp-554886) | 0.5358 | 0.001 | 4 |
BaMo2P3O14 (mp-640584) | 0.5705 | 0.000 | 4 |
Mo4O11 (mp-565865) | 0.7287 | 0.008 | 2 |
Re2P2O11 (mp-647218) | 0.5639 | 0.000 | 3 |
As2W2O11 (mp-504532) | 0.6449 | 0.027 | 3 |
P2W2O11 (mp-566939) | 0.6582 | 0.009 | 3 |
Mo2P2O11 (mp-25668) | 0.5857 | 0.003 | 3 |
Mo2P3O13 (mp-585184) | 0.6549 | 0.000 | 3 |
Nb2Hg3S(O2F5)2 (mp-541093) | 0.6428 | 0.000 | 5 |
Ta2Hg3S(O2F5)2 (mp-541094) | 0.6263 | 0.000 | 5 |
NaNb4Tl3P2O17 (mp-556062) | 0.6749 | 0.000 | 5 |
KBaYSi2O7 (mp-559670) | 0.6450 | 0.000 | 5 |
K2ScSi4O10F (mp-557777) | 0.7081 | 0.000 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.7339 | 0.119 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points4 |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nb_pv Te P O |
Final Energy/Atom-7.2967 eV |
Corrected Energy-745.4329 eV
-745.4329 eV = -700.4863 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)