Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.055 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.223 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap4.969 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP23 [195] |
HallP 2 2 3 |
Point Group23 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 309.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 77.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 109.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 77.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 109.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 218.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 154.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 109.4 |
BN (mp-984) | <0 0 1> | <1 1 0> | 109.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 232.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 309.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 154.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 109.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 309.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 232.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 109.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 309.3 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 133.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 218.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 232.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 77.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 133.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 309.3 |
Au (mp-81) | <1 1 0> | <1 1 0> | 218.7 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 154.6 |
C (mp-48) | <0 0 1> | <1 0 0> | 232.0 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 154.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 309.3 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 309.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 309.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 77.3 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 109.4 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 309.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 218.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 154.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 154.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 77.3 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 109.4 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 77.3 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 309.3 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 309.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 154.6 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 77.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 109.4 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 133.9 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 232.0 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 77.3 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 232.0 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 109.4 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 154.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.01438 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.01438 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.01438 |
Piezoelectric Modulus ‖eij‖max0.01438 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.97 | 0.00 | 0.00 |
0.00 | 1.97 | 0.00 |
0.00 | 0.00 | 1.97 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.22 | 0.00 | 0.00 |
0.00 | 3.22 | 0.00 |
0.00 | 0.00 | 3.22 |
Polycrystalline dielectric constant
εpoly∞
1.97
|
Polycrystalline dielectric constant
εpoly
3.22
|
Refractive Index n1.40 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsAuO3 (mp-755240) | 0.5236 | 0.117 | 3 |
H2SeO4 (mp-23866) | 0.7061 | 0.000 | 3 |
VBO4 (mp-771386) | 0.7161 | 0.068 | 3 |
TlP(HO2)2 (mp-697267) | 0.6967 | 0.000 | 4 |
SiO2 (mp-554665) | 0.4235 | 0.199 | 2 |
SiO2 (mp-556132) | 0.4526 | 0.191 | 2 |
SiO2 (mp-556880) | 0.4489 | 0.146 | 2 |
CeSe2 (mp-1080865) | 0.3200 | 0.526 | 2 |
CeSe2 (mp-1080366) | 0.3605 | 0.516 | 2 |
RbB2P2HO9 (mp-758281) | 0.6390 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.6934 eV |
Corrected Energy-293.8168 eV
-293.8168 eV = -276.9619 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)