Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.620 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgSbS2 + PbS |
Band Gap1.099 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 233.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 233.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 235.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 233.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 327.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 233.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 298.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 298.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 235.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 273.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 186.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 182.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 313.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 327.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 313.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 156.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 235.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 327.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 140.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 156.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 327.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 327.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 235.0 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 273.6 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 91.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 273.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 327.1 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 273.6 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 235.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 327.1 |
BN (mp-984) | <1 1 0> | <1 0 0> | 99.3 |
BN (mp-984) | <1 1 1> | <0 1 0> | 233.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 219.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 186.9 |
Al (mp-134) | <1 0 0> | <0 1 0> | 327.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 327.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 313.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 327.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 327.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 99.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 235.0 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 91.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 219.5 |
LiTaO3 (mp-3666) | <1 0 1> | <1 1 0> | 219.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 78.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 273.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 182.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 78.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 235.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 327.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GdAsO3 (mp-753953) | 0.6124 | 0.055 | 3 |
V(ZnN)2 (mvc-15550) | 0.5642 | 0.455 | 3 |
Na2PbO2 (mp-27622) | 0.5851 | 0.000 | 3 |
AgAsS2 (mp-542609) | 0.5297 | 0.010 | 3 |
Na2SnO2 (mp-778057) | 0.5752 | 0.000 | 3 |
KHgSbS3 (mp-6678) | 0.7221 | 0.011 | 4 |
Ag2Hg(SeO3)2 (mp-558763) | 0.6925 | 0.012 | 4 |
KLi2Mn2O4 (mp-780874) | 0.5824 | 0.080 | 4 |
SrLi3MnN3 (mp-570931) | 0.7159 | 0.047 | 4 |
AgAsPbS3 (mp-22665) | 0.4333 | 0.000 | 4 |
MoN2 (mvc-13455) | 0.7422 | 0.267 | 2 |
MgSi2 (mp-1073358) | 0.6537 | 0.177 | 2 |
MgSi2 (mp-1073644) | 0.7289 | 0.163 | 2 |
GeO2 (mp-20893) | 0.6856 | 1.555 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Sb Pb_d S |
Final Energy/Atom-4.1353 eV |
Corrected Energy-107.2096 eV
-107.2096 eV = -99.2481 eV (uncorrected energy) - 7.9615 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)