Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.811 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY3Al5O12 + Y2O3 |
Band Gap4.361 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 0 1> | 234.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 234.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 234.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 118.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 234.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 156.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 156.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 156.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 234.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 161.1 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 161.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 312.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 312.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 156.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 161.1 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 234.3 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 237.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 234.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 222.5 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 234.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 158.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 234.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 78.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 111.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 234.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 156.2 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 312.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 156.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 156.2 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 234.3 |
WS2 (mp-224) | <1 0 0> | <1 1 1> | 179.5 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 234.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 1> | 222.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 0 1> | 156.2 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 78.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 234.3 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 312.4 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 161.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 234.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 156.2 |
C (mp-66) | <1 1 0> | <1 0 1> | 161.1 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 118.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 312.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 312.4 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 156.2 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 316.8 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 158.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 316.8 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 312.4 |
Au (mp-81) | <1 1 0> | <0 1 1> | 222.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
204 | 83 | 80 | 0 | -5 | 0 |
83 | 216 | 71 | 0 | 1 | 0 |
80 | 71 | 213 | 0 | -9 | 0 |
0 | 0 | 0 | 73 | 0 | -3 |
-5 | 1 | -9 | 0 | 68 | 0 |
0 | 0 | 0 | -3 | 0 | 66 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.4 | -1.9 | -1.7 | 0 | 0.2 | 0 |
-1.9 | 5.8 | -1.2 | 0 | -0.4 | 0 |
-1.7 | -1.2 | 5.8 | 0 | 0.7 | 0 |
0 | 0 | 0 | 13.7 | 0 | 0.7 |
0.2 | -0.4 | 0.7 | 0 | 14.9 | 0 |
0 | 0 | 0 | 0.7 | 0 | 15.2 |
Shear Modulus GV68 GPa |
Bulk Modulus KV122 GPa |
Shear Modulus GR67 GPa |
Bulk Modulus KR122 GPa |
Shear Modulus GVRH68 GPa |
Bulk Modulus KVRH122 GPa |
Elastic Anisotropy0.04 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Lu4Al2O9 (mp-780420) | 0.4726 | 0.033 | 3 |
Lu4Al2O9 (mp-780406) | 0.1234 | 0.036 | 3 |
La4Al2O9 (mp-781707) | 0.4735 | 0.000 | 3 |
Y4Ga2O9 (mp-769481) | 0.3982 | 0.021 | 3 |
Y4Al2O9 (mp-5409) | 0.3622 | 0.012 | 3 |
Ca3HfSi2O9 (mp-15003) | 0.6832 | 0.000 | 4 |
Ca3Si2SnO9 (mp-15095) | 0.6829 | 0.000 | 4 |
Ca4Si2O7F2 (mp-560163) | 0.7014 | 0.000 | 4 |
Ca3ZrSi2O9 (mp-15004) | 0.6974 | 0.000 | 4 |
Ca7NbSi4O17F (mp-542863) | 0.7100 | 0.000 | 5 |
Y4AlSiNO8 (mp-1020714) | 0.6461 | 0.014 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Al O |
Final Energy/Atom-8.5824 eV |
Corrected Energy-540.2293 eV
-540.2293 eV = -514.9469 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction)
|