Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.972 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(PO3)2 |
Band Gap5.801 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 139.1 |
BN (mp-984) | <1 0 1> | <0 1 0> | 284.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 284.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 284.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 284.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 139.1 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 189.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 284.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 284.1 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 139.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 284.1 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 284.1 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 189.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 168.2 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 284.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2P4O13 (mp-770376) | 0.7267 | 0.179 | 3 |
Bi(PO3)3 (mp-27135) | 0.7397 | 0.000 | 3 |
Sr2P6O17 (mp-27583) | 0.7469 | 0.000 | 3 |
Ca4P6O19 (mp-559537) | 0.5946 | 0.000 | 3 |
Sn(PO3)3 (mp-26172) | 0.7380 | 0.088 | 3 |
LiSb(PO3)4 (mp-761773) | 0.7035 | 0.060 | 4 |
LiBi(PO3)4 (mp-759141) | 0.5653 | 0.063 | 4 |
LiTi(PO3)4 (mp-758056) | 0.7083 | 0.104 | 4 |
K2Ca4Si8O21 (mp-1019746) | 0.6900 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv P O |
Final Energy/Atom-7.2275 eV |
Corrected Energy-553.3584 eV
Uncorrected energy = -520.3824 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Corrected energy = -553.3584 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)