Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.263 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.551 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si(CN2)2 (mp-30160) | 0.5812 | 0.028 | 3 |
Be(CN)2 (mp-35687) | 0.5804 | 0.226 | 3 |
AlPO4 (mp-545974) | 0.4732 | 0.011 | 3 |
AlPO4 (mp-675254) | 0.5855 | 0.012 | 3 |
Mg2ZnN2 (mp-1029265) | 0.5512 | 1.954 | 3 |
LiB(CN)4 (mp-13590) | 0.6699 | 0.336 | 4 |
CuB(CN)4 (mp-13589) | 0.6270 | 0.351 | 4 |
CsAlSiO4 (mp-561457) | 0.6747 | 0.000 | 4 |
LiCo(CO)4 (mp-18939) | 0.6322 | 0.407 | 4 |
CsBePO4 (mp-15395) | 0.6779 | 0.000 | 4 |
CrN2 (mp-1014342) | 0.1543 | 0.338 | 2 |
CrN2 (mp-1015780) | 0.1491 | 0.340 | 2 |
CrN2 (mp-1097042) | 0.1472 | 0.337 | 2 |
CrN2 (mp-1097738) | 0.1591 | 0.339 | 2 |
CeSe2 (mp-1100189) | 0.0497 | 0.530 | 2 |
C (mp-1095534) | 0.6744 | 1.121 | 1 |
C (mp-1095633) | 0.7265 | 0.997 | 1 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9010 eV |
Corrected Energy-853.6595 eV
-853.6595 eV = -805.9038 eV (uncorrected energy) - 47.7557 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)