Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.142 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnS |
Band Gap2.032 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 321.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 270.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 192.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 205.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 360.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 205.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 282.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 321.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 291.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 167.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 270.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 115.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 347.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 270.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 167.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 257.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 372.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 270.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 308.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 205.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 270.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 192.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 115.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 205.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 257.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 334.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 270.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 192.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 90.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 205.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 347.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 167.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 270.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 192.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 90.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 128.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 308.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 360.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 270.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 167.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.02529 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.02529 | 0.00000 | 0.00000 |
-0.05309 | -0.05309 | 0.06361 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.09840 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-1.00000 |
-0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.87 | 0.00 | -0.00 |
0.00 | 5.87 | 0.00 |
-0.00 | 0.00 | 5.89 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.20 | 0.00 | 0.00 |
0.00 | 9.20 | 0.00 |
0.00 | 0.00 | 9.33 |
Polycrystalline dielectric constant
εpoly∞
5.88
|
Polycrystalline dielectric constant
εpoly
9.24
|
Refractive Index n2.42 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si3NiP4 (mp-8311) | 0.1893 | 0.000 | 3 |
Cu2SiTe3 (mp-675120) | 0.1900 | 0.001 | 3 |
Li3SbS4 (mp-760415) | 0.1840 | 0.005 | 3 |
GaCuTe2 (mp-3839) | 0.1910 | 0.000 | 3 |
CrCd3Te4 (mp-1079533) | 0.1871 | 0.115 | 3 |
CoCu2SiS4 (mp-556830) | 0.1792 | 0.065 | 4 |
ZnCu2GeS4 (mp-6408) | 0.1678 | 0.000 | 4 |
CoCu2SiS4 (mp-11769) | 0.1760 | 0.065 | 4 |
ZnCu2SiTe4 (mp-1078498) | 0.1831 | 0.000 | 4 |
LiIn2CuSe4 (mp-1079491) | 0.1856 | 0.004 | 4 |
ZnS (mp-554999) | 0.0030 | 0.001 | 2 |
ZnS (mp-557151) | 0.0044 | 0.012 | 2 |
ZnS (mp-554630) | 0.0028 | 0.001 | 2 |
ZnS (mp-555583) | 0.0028 | 0.001 | 2 |
ZnS (mp-556468) | 0.0044 | 0.012 | 2 |
C (mp-611448) | 0.0295 | 0.143 | 1 |
C (mp-616440) | 0.0221 | 0.141 | 1 |
C (mp-569517) | 0.0406 | 0.145 | 1 |
C (mp-569567) | 0.0217 | 0.144 | 1 |
Ge (mp-1091415) | 0.0750 | 0.008 | 1 |
Explore more synthesis descriptions for materials of composition ZnS.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn S |
Final Energy/Atom-3.5085 eV |
Corrected Energy-61.4442 eV
-61.4442 eV = -56.1365 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)